A large number of binder ingredients such as cement and active mineral admixtures are used in the preparation of high-strength concrete, and the water:binder ratio is extremely low. This leads to a large amount of shrinkage of concrete at the early stage of curing, which poses a great threat to the safety and durability of the structure. To solve the cracking problem of high-strength concrete induced by high shrinkage, we choose to change the admixture to solve it. In this study, a high-performance expansion agent (HPEA) and shrinkage-reducing agent, which are currently studied in a small number, were selected by changing the way of admixture, and their effects on the strength and shrinkage of high-strength concrete were compared and analyzed. The results show that the addition of a HPEA is beneficial to the compressive strength of concrete and sufficient expansion can be obtained by using a high amount of HPEA, but there is an excessive and delayed expansion to produce cracks in the later stage. A shrinkage-reducing agent plays an adverse role in the development of concrete strength, but it performs better in inhibiting shrinkage. The combination of a HPEA and shrinkage reducing agent can largely avoid the formation of cracks, and the two have a certain synergy. The main reason is that a HPEA compensates for some of the negative effects of a shrinkage-reducing agent on concrete strength, and the shrinkage-reducing agent further strengthens the inhibition effect of a HPEA on concrete shrinkage, and to some extent avoids the risk of cracks caused by delayed expansion caused by admixture problems.
Prefabricated pavement, with its advantages of a high paving speed, low material consumption, low carbon emissions, high strength, and easy construction, has gradually been used to address issues associated with traditional cement pavement construction. However, even under the long-term combined effects of vehicle loads and environmental loads, the joints between pavement slabs remain prone to various problems. This paper proposes the use of steel-fiber-reinforced self-stressing concrete (SFRSSC) with a certain level of self-stress for joint pouring and connection to control the development of cracks in the joints and achieve seamless integration between the slabs. Additionally, the self-stress generated by SFRSSC is utilized to enhance the continuity of the prestressed design in precast slabs, thereby extending their service life. Through laboratory experiments and field tests, the self-stress magnitude, mechanical strength, and long-term applicability of SFRSSC were studied. The results indicate that SFRSSC can achieve self-stress levels of over 7 MPa under standard curing conditions, but the values decrease significantly when removed from the standard curing environment. SFRSSC exhibits a compressive strength of over 60 MPa and a flexural strength of over 9 MPa, both of which exceed the requirements of the relevant standards, making it suitable for use as a pavement joint material. During long-term monitoring in the field, SFRSSC demonstrates favorable expansion effects and high stability. The longitudinal expansion remains stable at 100 με, while the transverse expansion exhibits minor shrinkage, maintained at around 25.2 με. Therefore, the application of SFRSSC in assembly-type prestressed pavement joints shows high applicability.