Laser directed energy deposition (LDED) can be deployed for depositing high-performance materials for various engineering applications. Alumina-forming steel is a high-performance material that possesses excellent corrosion and oxidation resistance, finding application in the power generation sector. In the present work, LDED using powder feeding (LDED-PF) was used to deposit Fe20Cr5.5AlY alloy using single-track, multi-track, and multi-layer deposition on SS 316L substrate. Response surface methodology (RSM)-based optimization was used to optimize the single-track deposition. The relationship between the track geometry parameters and the build rate with the LDED-PF processing parameters was studied. Further, the nonlinear relationship among the major process parameters was developed and an analysis of variance (ANOVA) was utilized to find significant parameters. The multi-track deposition yielded densely clad layers with a columnar grain structure. The presence of complex oxide slag of Y, Al, and Zr on the clad layer was detected. A micro-hardness of 240–285 HV was observed in the clad layer, with a hardness of 1088–1276 HV at the slag layer. The multi-layered structures showed a relative density of 99.7% with columnar growth and an average microhardness of 242 HV. The study paves the way for the deposition of dense alumina-forming steel structures for building components for power generation applications.
Laser-Directed Energy Deposition (LDED) has recently been widely used for 3D-printing metal components and repairing high-value parts. One key performance indicator of the LDED process is represented by melt pool stability and spatter behavior. In this research study, an off-axis vision monitoring system is employed to characterize spatter formation based on different anomalies in the process. This study utilizes a 1 kW fiber laser-based LDED system equipped with a monochrome high-dynamic-range (HDR) vision camera and an SP700 Near-IR/UV Block visible bandpass filter positioned at various locations. To extract meaningful features from the original images, a novel image processing algorithm is developed to quantify spatter counts, orientation, area, and distance from the melt pool under harsh conditions. Additionally, this study analyzes the average number of spatters for different laser power settings, revealing a strong positive correlation. Validation experiments confirm over 93% detection accuracy, underscoring the robustness of the image processing pipeline. Furthermore, spatter detection is employed to assess the impact of spatter formation on deposition continuity. This research study provides a method for detecting spatters, correlating them with LDED process parameters, and predicting deposit quality.