Exergy destruction associated with the operation of a solar heating system is evaluated numerically via an exergy cascade. As expected, exergy destruction is dominated by heat transfer across temperature differences. An energy analysis is also given for comparison of exergy cascade to energy cascade. Efficiencies based on both the first law and second law of thermodynamics are calculated for a number of components and for the system. The results show that high first-law efficiency does not mean high second-law efficiency. Therefore, the second-law analysis has been proven to be a more powerful tool in identifying the site losses. The procedure used to determine total exergy destruction and second law efficiency can be used in a conceptual design and parametric study to evaluate the performance of other solar heating systems and other thermal systems.
In this study, a NiCoCrW (K447A) superalloy was fabricated using selective laser melting (SLM). The hot-corrosion behaviour of the SLM-fabricated NiCoCrW (K447A) was investigated in Na2SO4 at 900 °C. Microstructural analysis and hot-corrosion testing revealed its anisotropic behaviour in different build directions. The corrosion resistance along the build direction (XOY plane) was superior to that perpendicular to the build direction (YOZ plane). The stability of grain boundaries in the XOY plane is enhanced by the fine grains and a larger carbide area fraction, effectively hindering the diffusion of S and O2 at grain boundaries. Furthermore, the more uniform distribution of carbides in the XOY plane reduces the local stress concentration, contributing to the stability of the protective oxide film. The enhanced hot-corrosion resistance is attributed to the formation of a more continuous and dense corrosion layer on the XOY surface.
In this study, systematic heat treatment routes including solution (980 °C to 1130 °C) and aging (675 °C to 775 °C) processes were used to tailor the microstructural evolution and mechanical performance of a Fe-Ni-Cr based austenitic alloy, strengthened by a γ′ phase (Ni3(Ti, Al)). Grain growth was observed with increasing solution treatment temperature from nearly 90 μm (980 °C) to nearly 200 μm (1130 °C). Grain refinement during solution heat processes was found to ascribe to the solute drag effect and the pinning effect of nickel-titanium-enriched segregates and precipitates. During aging, the precipitation behavior of γ′ is found to be almost independent of solution treatment temperatures. Interestingly, abnormal grain growth during aging was observed. The motion of grain boundaries was ascribed to the formation of nickel-titanium-enriched γ′ in the austenitic matrix, thereby contributing to the dissolution of the previously enriched segregates and precipitates from grain boundaries. The studied alloy shows a wide range of mechanical properties, from tensile strength of 1131 MPa with ductility at 36%, to tensile strength of 880 MPa with ductility at 50%. The current study demonstrates that grain refinement of the alloy at solution treatment may not benefit the final mechanical properties.