Combining dissimilar parts has become imperative for developing the structures based on lightweight materials, such as metal alloys, polymers or polymer matrix composites, and this has become one of the solutions to reverse the current trend of CO2 emissions in the transport sector. However, given the usual property disparities, joining dissimilar materials in multi-material and multi-purpose structures raises new engineering challenges. Advanced joining processes, such as friction stir welding (FSW), have emerged and have been applied across several sectors as a promising alternative to conventional joining processes, such as mechanical fastening or adhesive bonding. In the present work, and in order to avoid the development of intermetallic compounds (IMCs), a different approach from the conventional technique of friction stir welding was applied to the production of dissimilar overlapping joints. These dissimilar joints were fabricated using a high strength aluminum alloy (AA7075-T651) and a titanium alloy (Ti-6Al-4V), both materials widely used in automotive, aeronautics and space industries. To perform a systematic investigation, the Taguchi method was used to determine the process parameter combinations to enable the fabrication of this type of dissimilar joints. The joints were subjected to quasi-static tensile shear tests to assess their mechanical performance and were compared to conventionally riveted joints in different configurations, namely, single and double connection points. The joints produced by the FSW based method showed higher mechanical performance. To assess the local properties, some of the fractured regions of the joints were subjected to hardness assessments, revealing no significant change in the hardness in the tested areas. Finally, a statistical study was performed to analyze the main effects and interactions of the process parameters, to identify their influences on the mechanical performance of the joints.
With the increasing demand for lighter, more environmentally friendly, and affordable solutions in the mobility sector, designers and engineers are actively promoting the use of innovative integral dissimilar structures. In this field, friction stir-based technologies offer unique advantages compared with conventional joining technologies, such as mechanical fastening and adhesive bonding, which recently demonstrated promising results. In this study, an aluminum alloy and a glass fiber-reinforced polymer were friction stir joined in an overlap configuration. To assess the main effects, interactions, and influence of processing parameters on the mechanical strength and processing temperature of the fabricated joints, a full factorial design study with three factors and two levels was carried out. The design of experiments resulted in statistical models with excellent fit to the experimental data, enabling a thorough understanding of the influence of rotational speed, travel speed, and tool tilt angle on dissimilar metal-to-polymer friction stir composite joints. The mechanical strength of the composite joints ranged from 1708.1 ± 45.5 N to 3414.2 ± 317.1, while the processing temperature was between 203.6 ± 10.7 °C and 251.5 ± 9.7.
This work provides a detailed description of the procedures employed to characterize the mechanical behaviour of two materials present in a coach’s exterior panels, including glass-fibre-reinforced polymer (GFRP) and neat DCPD (dicyclopentadiene)-based polymers. Tensile tests were conducted at quasi-static, intermediate [1 s−1, 10 s−1], and high strain rates [150 s−1, 250 s−1] to obtain a comprehensive understanding of their behaviour. The results indicate positive and significant dependence on the strain rate. Additionally, GFRP demonstrates superior energy absorption capacity for higher strain rates, unlike DCPD, which exhibits a higher energy absorption capacity for QS tests. In the case of DCPD, raising the strain rate to 10 s−1 the maximum stress was not affected but decreased the elongation at fracture. At higher strain rates, there was an increase in maximum stress alongside greater elongation. DCPD maintained consistent stiffness across all rates ranging between 2087 MPa and 2389 MPa, and the tests disclosed a failure mode characterized by numerous surface-transverse fissures. Regarding GFRP, a more pronounced variation in stiffness is observed, decreasing from 11,005 MPa to 4532 MPa at 133 s−1, recovering to 7288 MPa at 252 s−1. In addition, the maximum stress and failure elongation tends to increase with the strain rate increase. The detailed analysis of these results provides valuable insights into the mechanical behaviour of these materials under different loading conditions.