Rubber from recycled car tires and styrene-butadiene-styrene (SBS) were used for the chemical modification of commercially available road bitumen 50/70 (EN 12591). The modification process began with the addition of rubber into asphalt and heating the whole amount at the temperature of 190 °C or 220 °C. Under such conditions, de-vulcanization of rubber took place. Next, SBS and sulfur as a cross-linker were added and the heating was continued so that cross-linking of SBS and the de-vulcanized rubber proceeded. In the studies on the influence of rubber concentration on the final properties of asphalt 10% or 15% of rubber was considered. Chemical modification reactions were performed within 2, 4, and 8 h. The results showed that both the modification at 190 °C and 220 °C affected the properties of the base asphalt efficiently, although the asphalt modified at 190 °C contained more non-degraded rubber. Increasing the modification time led to dissolution of the rubber crumbs and its de-vulcanization. Bitumens modified in this way are characterized by high storage stabilities. Their behavior at low temperatures also deserves attention.
12 April 2021 in Road Materials and Pavement Design
The paper briefly discusses traditional asphalt pavements designing methods of designing of asphalt pavements developed in the second half of the 20th century. In comparison, it presents the assumptions and derivations of a modern method based on the simplified viscoelastic continuum damage (S-VECD) model together with its necessary input data. In the second part of the article, structures for two different traffic load categories - heavy traffic and extreme traffic - were analysed. For each traffic load categories two types of constructions were compared - reference construction - made with typical neat asphalt binder in base course and construction with anti-fatigue base layer made with highly polymer modified asphalt binder (HiMA). Fatigue performance of each structure was estimated using two methods - Asphalt Institute method and S-VECD method. Results showed that approach using the Asphalt Institute equations is correct for unmodified asphalt materials, while for the asphalt mixtures with a high elastomer content it generates rather doubtful results. The example presented that it is possible the possibility of to captureing the field performance of HiMA with the S-VECD method.
Since 2009, SBS (styrene-butadiene-styrene) polymer-modified binders (HiMA—Highly Modified Asphalt) have been tested worldwide. Highly modified binders are characterized by extraordinary properties resulting from the reversal of the binder-polymer phase. This contributes to very good test results for asphalt mixes. The use of such a modern binder poses a challenge in terms of structure design, mainly due to the lack of a recognized and calibrated method suitable for this material. The article proposes a new approach to pavement fatigue life estimation—the Similarity Method—which is based on the use of AASHTO 2004 equations and laboratory fatigue testing results of asphalt concrete mixes for asphalt base course. The article presents the method and the results of its sensitivity testing with respect to the influence of the material (type of asphalt concrete), thickness of the asphalt base course, stiffness of the subgrade and the assumed FC index (the area of bottom-up cracks). The results of fatigue life according to the Similarity Method are within the range of values obtained for AASHTO 2004 and the fatigue results according to the equations obtained in the laboratory. This approach will enable inclusion of new materials, such as HiMA asphalt mixtures, in pavement structure design.
The aim of the study is to compare flexible pavement design lifespans and the main factors which create their values for a standard structure and one with an anti-fatigue course AF at different parameter values of pavement and its load, relevant to their design processes. Depending on the mixture used for the anti-fatigue course or the course thickness, durability improvement of the pavement (compared to the durability of a standard structure) can be obtained by extending the design lifespan of the asphalt base course or by extending the design lifespan of the AF course. On sections with predominantly slow traffic, the lifespan decreases significantly compared to sections with typical vehicle speed-the relative decrease is greater if anti-fatigue course is applied.
Postęp technologiczny i wprowadzenie do stosowania zaawansowanych materiałów o ponadstandardowych właściwościach, np. mieszanek mineralno-asfaltowych z lepiszczami wysokomodyfikowanymi polimerami HiMA (ang. highly modified asphalt), wymaga poszukiwania metody umożliwiającej kompleksowe uwzględnienie cech tych materiałów w obliczeniach. Jedną z takich metod może być metoda wykorzystująca model rozproszonego niszczenia w ośrodku lepkosprężystym (ang. viscoelastic continuum damage model, VECD). W artykule zaprezentowano metodologię opartą na modelu VECD oraz możliwości, jakie daje przy wymiarowaniu nawierzchni drogowych. Opisano poszczególne komponenty metody: analogię sprężysto-lepkosprężystą, mechanikę rozproszonego niszczenia i zasadę równoważności temperaturowo-czasowej z przyrostowym niszczeniem. Przedstawiono rów¬nież koncepcję uproszczonych obliczeń w metodzie S-VECD (ang. simplified viscoelastic continuum damage model). Artykuł zawiera opisy opracowanych kryteriów zniszczenia. Przybliżono również metody badań, które dostarczają danych wejściowych. W końcowej części artykułu przedstawiono przykładową analizę porównawczą z wykorzystaniem metody S-VECD dla konstrukcji z mieszankami mineralno-asfaltowymi z HiMA w warstwie podbudowy i mieszankami mineralno-asfaltowymi z HiMA we wszystkich warstwach.