Calcium carbide residue (CCR) is a waste by-product from acetylene gas production. The main component of CCR is Ca(OH)2, which can react with siliceous materials through pozzolanic reactions, resulting in a product similar to those obtained from the cement hydration process. Thus, it is possible to use CCR as a substitute for Portland cement in concrete. In this research, we synthesized CCR and silica fume through a chemical combustion technique to produce a new reactive cementitious powder (RCP). The properties of paste and mortar in fresh and hardened states (setting time, shrinkage, and compressive strength) with 5% cement replacement by RCP were evaluated. The hydration of RCP and OPC (Ordinary Portland Cement) pastes was also examined through SEM (scanning electron microscope). Test results showed that in comparison to control OPC mix, the hydration products for the RCP mix took longer to formulate. The initial and final setting times were prolonged, while the drying shrinkage was significantly reduced. The compressive strength at the age of 45 days for RCP mortar mix was found to be higher than that of OPC mortar and OPC mortar with silica fume mix by 10% and 8%, respectively. Therefore, the synthesized RCP was proved to be a sustainable active cementitious powder for the strength enhanced of building materials, which will result in the diversion of significant quantities of this by-product from landfills.
C-A-S-H (CaO-Al2O3-SiO2-H2O) and N-A-S-H (Na2O-Al2O3-SiO2-H2O) have a wide range of chemical compositions and structures and are difficult to separate from alkali-activated materials. Therefore, it is difficult to analyze their microscopic properties directly. This paper reports research on the synthesis of C-A-S-H and N-A-S-H particles with an average particle size smaller than 300 nm by applying the hydrothermal method. The composition and microstructure of the products with different CaO(Na2O)/SiO2 ratios and curing conditions were characterized using XRD, the RIR method, FTIR, SEM, TEM, and laser particle size analysis. The results showed that the C-A-S-H system products with a low CaO/SiO2 ratio were mainly amorphous C-A-S-H gels. With an increase in the CaO/SiO2 ratio, an excess of Ca(OH)2 was observed at room temperature, while in a high-temperature reaction system, katoite, C4AcH11, and other crystallized products were observed. The katoite content was related to the curing temperature and the content of Ca(OH)2 and it tended to form at a high-temperature and high-calcium environment, and an increase in the temperature renders the C-A-S-H gels more compact. The main products of the N-A-S-H system at room temperature were amorphous N-A-S-H gels and a small amount of sodalite. An increase in the curing temperature promoted the formation of the crystalline products faujasite and zeolite-P. The crystallization products consisted of only zeolite-P in the high-temperature N-A-S-H system and its content were stable above 70%. An increase in the Na2O/SiO2 ratio resulted in more non-bridging oxygen and the TO4 was more isolated in the N-A-S-H structure. The composition and microstructure of the C-A-S-H and N-A-S-H system products synthesized by the hydrothermal method were closely related to the ratio of the raw materials and the curing conditions. The results of this study increase our understanding of the hydration products of alkali-activated materials.
The relatively high shrinkage of the alkali-activated slag (AAS) has restricted its application as a widely-used building material. This research attempts to study the effect of a hydrothermally synthesized C-A-S-H gel, which has a similar composition to that of the main AAS product, on the shrinkage performance of the AAS. The C-A-S-H nano-particles were mixed into AAS mortars in a proportion ranging from 1 wt % to 5 wt % using two different methods, and the drying and autogenous shrinkage ratio of modified AAS mortars were measured at various ages. The effect of C-A-S-H on their microstructures was also characterized. Results obtained indicated that the addition of C-A-S-H gel to AAS mortars had reduced their drying and autogenous shrinkage, with the addition of 3 wt % reaching the maximum reduction. However, the added amount was not directly proportional to the decrease of shrinkage; the proportion of early-stage drying shrinkage of AAS mortars was greater than that of autogenous shrinkage; the dispersion method was slightly better than the dry mixing method in both shrinkage reduction. MIP results suggested that the addition of C-A-S-H gel had reduced the total porosity and the average pore size of AAS mortars, optimized their pore structure distribution, and significantly reduced the volume of mesopores (<0.05 µm) which resulted in high shrinkage, while the adding method had no significant effect on the pore size distribution of AAS mortars. SEM results showed that the addition of C-A-S-H gel can reduce the crack width of mortars, obtain a dense and uniform matrix structure, increase the density, and effectively suppress both shrinkage deformation of the system, whereas the adding method has no obvious effect on the crack width of the mortar. This research provides a novel approach of the AAS shrinkage reduction and structure refinement, shedding lights on nano-material modification of the AAS.
This study investigated the influence of alkali content on the early-age hydration process of slag-based geopolymer and the feasibility of non-destructive resistivity. Results showed that there existed a threshold of alkali content in adjusting the early-age hydration. Initially, increasing the alkali content tended to accelerate the dissolution period (detected by resistivity and heat release rate) and resulted in a denser microstructure (detected by TEM). When the alkali content surpassed 6 wt%, the increasing alkali content mitigated the structural development of a slag-based geopolymer, as it lowered the liquid water content and caused local precipitation, which trapped the early-age ions transmission and, therefore, the later-age mechanical development was inhibited. It was proven that the resistivity acted as a linkage among the reaction degree, workability, and strength development.
In the interest of solving the resource and environmental problems of the construction industry, low-carbon geopolymer coating ensures great durability and extends the service life of existing infrastructure. This paper presents a multidisciplinary assessment of the protective performance and environmental impacts of geopolymer coating. Various parameters, such as main substance, water-solid (W/S) ratio, activator type and curing time, were investigated for their effects on interface characterization in terms of contact angle, surface energy, mechanical properties and microstructure. These parameters had negligible effects on the amounts and types of hydrophilic functional groups of geopolymer surfaces. A combination of organic surface modifiers and geopolymer coatings was shown to ensure hydrophobic surface conditions and great durability. Silicon-based modifiers exhibited better wetting performance than capillary crystalline surfactants by eliminating hydroxyl groups and maintaining structural backbone Si-O-T (Si, Al) on geopolymers’ surfaces. Finally, life-cycle analysis was conducted to investigate the environmental performance. Geopolymer coating yielded substantially lower environmental impacts (50–80% lower in most impact categories) than ordinary Portland cement (OPC) coating. Silicon-based modifiers had negligible influence due to their minimal usage. Increasing the W/S ratio diluted the geopolymer coating and decreased the environmental impacts, and slag-based geopolymer coating achieved lower environmental impacts than FA-based and MK-based varietie.
K-A-S-H (K2O-Al2O3-SiO2-H2O) gel is a key phase that forms in most alkali-activated binders (eco-friendly binders which utilize a substantial amount of industrial by-product). An in-depth understanding of the microstructure and performance of this nano-sized key phase facilitates better application to alkali-activated binders. However, such studies remain little and undetailed. Therefore, our research aims to provide insights into the microstructure of K-A-S-H particles synthesized with accurate stoichiometric control by the hydrothermal method through thermogravimetric analysis (TG), Fourier transform infrared spectroscopy (FTIR), nuclear magnetic resonance (NMR), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and BET surface area. The results show that for materials prepared at the curing temperature lower than 80 °C, the K-A-S-H products were completely amorphous. With increased curing temperature and time, the K-A-S-H products were transformed from the amorphous phase to the crystalline zeolite phase structure, with a reduction in the specific surface area. The TG results indicate that the crystalline phase contains more non-evaporated water or zeolite water for structural rearrangement. The degree of tetrahedral polymerization slightly decreased with an increase of the K2O/SiO2 ratio as the amount of non-bridged oxygen atoms increased, whereas it gradually increased with an increase of curing temperature and time, as suggested by the FTIR and NMR results. Various K2O/SiO2 ratios resulted in the formation of zeolite K-H and K-G zeolite, both of which exhibited highly polymerized three-dimensional network structures. However, there was no significant effect of the SiO2/Al2O3 ratio on the structure of K-A-S-H products. Overall, these results provide insight into understanding the chemical stability of K-A-S-H.