Of the study was to analyse translucency parameter (TP values) of glass-ceramics fabricated by different techniques and investigate the effect of the corrosive medium on TP values. Three specimens of each type of IPS e.max ceramics (Ivoclar Vivadent, Schaan, Liechtenstein) were made in three colours (A2, C2 and B3) by three fabrication techniques (layering - e.max Ceram Dentin; heat-pressing - e.max Press; CAD/CAM - e.max CAD). Specimens were made in the form of plates (10 mm x 12 mm x 0.8 mm). CIE L*a*b* values were measured by a spectrophotometer (X-Rite DTP 20 Pulse, Neu Isenburg, Germany) before and after exposure to 4% acetic acid at 80 °C for 16 hours (ISO 6872) to calculate translucency parameter (TP values). Statistical data were analysed using the IBM SPSS 22 software. IPS e.max Ceram Dentin had significantly the lowest TP values, and IPS e.max Press the highest TP values of all colours (A2, C2, B3), both prior and after exposure to acid (p<0.001). The difference in TP values among colours was evident in the IPS e.max Ceram Dentin material, both before and after exposure to acid with a great effect size (p<0.001; η2 = 0.702 and 0.741), and in the IPS e.max Press material (p<0.001, effect size 0.547 and 0.576). CAD/CAD specimens showed uniform TP values between three colours. Further, exposure to a corrosive medium did not result in a statistically significant change of TP values in any of the materials tested. Different types of glass-ceramics showed significant difference in TP values both with respect to the fabrication technique and colour. Exposure to a corrosive medium did not result in a statistically significant change of TP values.
Objectives: To examine the effect of two aging protocols on the chemical and phase composition as well as the surface state of monolithic translucent zirconia ceramics. Material and Methods: Translucent zirconia ceramics KATANA-Zirconia STML with different surface treatments (no treatment, K1, K2; glazed, G1-G8; polished, P1-P8) underwent testing in order to examine how the two aging protocols (three-hour hydrothermal degradation in an autoclave at 134 °C and 2 bars: G1-G4, P1-P4, and sixteen-hour chemical degradation in four-percent acetic acid at 80 °C (ISO 6872): G5-G8, P5-P8) affect chemical composition, particularly the share of stabilizing yttrium oxide (Energy Dispersive XRay Fluorescence – EDXRF), phase composition (X-ray diffraction – XRD) and surface state in terms of roughness and gloss. Results: Aging protocols did not affect the tested chemical composition stability of specimens and a high share of stabilizing yttrium-oxide (≥10% of total content), which correlates with the absence of monoclinic phase. A decrease in gloss on all specimens is statistically significant. Chemical degradation substantially increased the surface roughness of tested specimens. Conclusions: Translucent monolithic zirconia demonstrated a stable chemical composition and resistance to tetragonal-to-monoclinic transformation. Surface gloss was significantly reduced, especially in polished specimens. Contrary to glazed specimens, the tested polished specimens manifested an increase in surface roughness. Glazing the surface of translucent monolithic zirconia produces better esthetic, tribological and hygienic effects than polishing.
Objectives: The development and placement of translucent zirconia ceramics on the dental materials market is in full swing. This research aimed to investigate how aging protocols affect the microstructure, color parameters and translucency of a new-generation monolithic zirconia ceramic. Material and methods: Translucent zirconia ceramics KATANA-Zirconia STML with different surface treatments (as sintered - control, glazed, polished) was tested using two aging protocols (hydrothermal degradation in autoclave at 134 degrees C and 2 bars for three hours, chemical degradation in four-percent acetic acid at 80 degrees C for 16 hours) in order to examine phase composition using X-ray diffraction analysis and Delta E, Delta L and Delta C color parameters through spectrophotometry. The translucency parameter (TP) was calculated using parameters L*, a* and b* on a black and white surface. Results: Regardless of the surface treatment, aging protocols did not cause a tetragonal-to-monoclinic phase transformation, although hydrothermal degradation in the autoclave transformed the hybrid tetragonal-cubic structure of all specimens to a tetragonal one. All polished and glazed specimens during chemical degradation demonstrated a significant color change Delta E. Lightness Delta L significantly changed in polished specimens aged in the autoclave. In all specimens, Delta C underwent a change manifested through statistically insignificant yellowing. None of the aging protocols altered the translucency of specimens. Conclusions: Aging, regardless of the final surface treatment, did not manifest a monoclinic phase in the specimens. A tetragonal-cubic microstructure dominates. Unlike polishing, glazing the surface of translucent zirconia ceramics contributed to minor changes in color, lightness and chromaticity. The translucency of translucent zirconia ceramics remains stable regardless of aging and surface treatment.