Titanium aluminides find application in modern light-weight, high-temperature turbines, such as aircraft engines, but suffer from poor plasticity during manufacturing and processing. Huge forging presses enable materials processing in the 10-GPa range, and hence, it is necessary to investigate the phase diagrams of candidate materials under these extreme conditions. Here, we report on an in situ synchrotron X-ray diffraction study in a large-volume press of a modern (α2 + γ) two-phase material, Ti-45Al-7.5Nb-0.25C, under pressures up to 9.6 GPa and temperatures up to 1686 K. At room temperature, the volume response to pressure is accommodated by the transformation γ → α2, rather than volumetric strain, expressed by the apparently high bulk moduli of both constituent phases. Crystallographic aspects, specifically lattice strain and atomic order, are discussed in detail. It is interesting to note that this transformation takes place despite an increase in atomic volume, which is due to the high ordering energy of γ. Upon heating under high pressure, both the eutectoid and γ-solvus transition temperatures are elevated, and a third, cubic β-phase is stabilized above 1350 K. Earlier research has shown that this β-phase is very ductile during plastic deformation, essential in near-conventional forging processes. Here, we were able to identify an ideal processing window for near-conventional forging, while the presence of the detrimental β-phase is not present under operating conditions. Novel processing routes can be defined from these findings.
In the present study, the isothermal decomposition of austenite to bainite in 1.0 wt% carbon, 0.21% silicon steel during the partitioning step of a quenching and partitioning (Q&P) heat treatment has been investigated in a dilatometer in the temperature range of 200 to 350 °C and compared to conventional austempering heat treatment. The bainite transformation was shortened by about 75% in the presence of pre-existing martensite (QP). The kinetics of bainite transformation is described by the well-known Avrami equation. The calculated parameter ‘n’ in the Avrami equation shows that bainite forms in the absence of pre-existing martensite (TT) at a constant nucleate rate, while in the presence of pre-existing martensite, nucleation is interface controlled. The overall bainite transformation activation energy, calculated by the Avrami equation, ranges from 64 to 110 kJ/mol. The outcomes of this investigation provide guidelines for the development of multiphase microstructures, including pre-existing martensite and bainite in high-carbon low-silicon steel, within an industrially acceptable time scale and mechanical performance.
26 September 2021 in Metallurgical and Materials Transactions A