The excessive utilization of petroleum-based plastic products has led to a pervasive environmental and human health threat. In response, the adoption of bioplastics derived from biomass has emerged as the foremost alternative to conventional plastics, owing to their inherent biodegradability and sustainability. The present study demonstrates the preparation of a biodegradable and cost-effective lignocellulosic bioplastic by utilizing dissolving bamboo leaf powder with deep eutectic solvents (DES) and regenerating lignin in situ. The DES was synthesized through a one-step heating and stirring method using choline chloride (ChCl) and anhydrous oxalic acid. The crystallinity of the bioplastics is enhanced by DES pretreatment, thereby improving the internal structural order of the material. Moreover, lignin regeneration reduces the pore size within the bioplastics and contributes to a more compact internal structure. The prepared lignocellulosic bioplastics exhibit remarkable mechanical strength, with a tensile strength of 113 MPa. Additionally, they demonstrate good water stability, as evidenced by a contact angle of 55.52°. Moreover, these bioplastics possess an exceptional biodegradability with a degradation rate exceeding 98% after 60 days. This study presents an innovative approach for the high-value utilization of bamboo leaf resources.
Gluconic acid has been increasingly in demand in recent years due to the wide applications in the food, healthcare and construction industries. Plant-derived biomass is rich in biopolymers that comprise glucose as the monomeric unit, which provide abundant feedstock for gluconic acid production. Gluconobacter oxydans can rapidly and incompletely oxidize glucose to gluconic acid and it is regarded as ideal industrial microorganism. Once glucose is depleted, the gluconic acid will be further bio-oxidized to 2-ketogluconic acid by Gluconobacter oxydans. The endpoint is difficult to be controlled, especially in an industrial fermentation process. In this study, it was found that the low pH environment (2.5~3.5) could limit the further metabolism of gluconic acid and that it resulted in a yield over 95%. Therefore, the low pH stress strategy for efficiently producing gluconic acid from biomass-derived glucose was put forward and investigated with enzymatic hydrolysate. As a result, 98.8 g/L gluconic acid with a yield of 96% could be obtained from concentrated corncob enzymatic hydrolysate that initially contained 100 g/L glucose with 1.4 g/L cells loading of Gluconobacter oxydans. In addition, the low pH stress strategy could effectively control end-point and decrease the risk of microbial contamination. Overall, this strategy provides a potential for industrial gluconic acid production from lignocellulosic materials.
4 March 2025 in Advanced Composites and Hybrid Materials
Enhancing the dispersibility and recoverability of powdered catalysts is essential for developing efficient and cost-effective photocatalytic systems. Herein, β-FeOOH nanoparticles were in-situ deposited on commercially available filter paper (FP) to construct paper-based composite material (β-FeOOH@FP). Results showed that the rod-like β-FeOOH nanoparticles were uniformly distributed in the FP matrix without destroying the crystalline structure of cellulose. The resulting β-FeOOH synthesized at 3 h presented the highest photoelectrochemical response and exhibited better suppression of electron–hole recombination, allowing more photogenerated electrons to participate in the reaction. The β-FeOOH@FP catalyst achieved a 94.1% photocatalytic degradation rate of tetracycline (TC) within 120 min compared to the pure β-FeOOH (42.2%) and FP (20.1%) under simulated visible light irradiation. Photocatalytic degradation kinetics also demonstrated that the rate constant of β-FeOOH@FP was 9.6 × 10−3 min−1, much higher than that of others. In addition, the resulting β-FeOOH@FP composite material exhibited excellent stability and reusability with a photocatalytic efficiency of over 90% after five cycles. These findings provide a simple and cost-effective strategy to improve the degradation performance of powdered semiconductor catalysts and pave a new way to develop cellulose-based nanocomposites with high photocatalytic efficiency.
In order to improve the utilization of alkali lignin (AL) as an effective component for ultraviolet (UV) shielding, demethylation and acetylation modification were carried out to improve the UV absorption performance of lignin. Then, lignin-based sunscreens were successfully prepared by mixing the modified lignin and commercial cream without UV shielding ingredients. The modified alkali lignin was comprehensively characterized in terms of its molecular weight, functional groups and structural properties by GPC, UV spectroscopy and 31P NMR. The results showed that the Mw of all three lignin feedstocks (AL, ALMeOH and ALAcetone) was decreased with prolonged demethylation time. Compared to the original feedstock, demethylated AL had a darker color and improved UV absorption performance due to the increased phenolic hydroxyl content (approximately 4.35 mmol/g). 31P-NMR spectra showed that the guaiacyl phenolic hydroxyl content decreased rapidly after acetylation, causing the sample color to become lighter. Among all lignin-based sunscreens, DALAcetone achieved the highest SPF value of 11.23, a 69.4% increase over its pre-reaction level and a 7.58-fold enhancement compared to the original lignin. In summary, this study opens a promising avenue for repurposing industrial lignin as a sustainable biomaterial in high-value sectors like UV-blocking agents and cosmetic formulations.
This study systematically investigated the pretreatment effects of diol-based DESs (deep eutectic solvents) on Pinus massoniana Lamb. (P. massoniana). A diol-based DES system (Choline chloride (ChCl): AlCl3: BDO) was developed to degrade and disassemble P. massoniana, thereby facilitating saccharification and achieving the utilization of high-value lignin. The DES-based pretreatment achieved a glucan recovery yield of 92.95% and a xylan yield of 71.73% at 130 °C. Meanwhile, the lignin removal yields reached 61.96% at 130 °C, and the lignin recovered from DES fractionation was also preserved well; moreover, the β-O-4′ linkage content was retained at approximately 51.63%. DES was also demonstrated to be promising for promoting cellulose saccharification, lignin fractionation and enzymatic hydrolysis. The preservation mechanism was speculated to involve the introduction of diol -OH groups at the Cα-position of the lignin β-O-4′ structure via etherification. In addition, FT-IR indicated that the main structure of cellulose in P. massoniana remained unchanged after pretreatment. The grafting of diol onto the Cα-position of the β-O-4′ linkages was confirmed by 2D-HSQC, which could inhibit lignin further condensation; 31P NMR revealed that the total phenolic -OH content increased significantly and was enhanced by pretreatment, which indicated that methoxy and ether bond groups were reduced.