This study investigated the bond behavior and radial crack between concrete and reinforcing bars using cold-drawn shape memory alloy (SMA) crimped fibers controlled by the temperature and volume fraction of the fibers. In this novel approach, the concrete specimens containing cold-drawn SMA crimped fibers with 1.0% and 1.5% volume fractions of cold-drawn SMA fibers were prepared. After that, the specimens were heated to 150 °C to generate recovery stress and activate prestressing within the concrete. The bond strength of specimens was estimated by pullout test using the universal testing machine (UTM). Furthermore, the cracking patterns were investigated using radial strain measured by a circumferential extensometer. The results showed that adding up to 1.5% of SMA fibers improved the bond strength by 47.9% and reduced radial strain by more than 54%. Thus, heating specimens containing SMA fibers showed improved bond behavior compared with non-heated specimens with the same volume fraction.
4 June 2026 in Composites Part A: Applied Science and Manufacturing
This study examines the influence of the geometry of mortar beams reinforced with crimped shape memory alloy fibers on flexural behavior using the mesoscale finite element method. Moreover, the shape memory effect induced by heating to prestressing inside the mortar matrix was simulated and considered in this model. To this end, 240 mesoscale beams were modeled using fibers with diameters ranging from 0.3 mm to 1.0 mm; lengths of 20.0 mm, 30.0 mm, and 40.0 mm; and volume fractions of fibers of 0.25%, 0.5%, 0.75%, 1.0%, and 1.25%. The results indicated that the flexural capacity and toughness of the beam were enhanced by increasing the volume fraction of the fibers. Additionally, increasing the fiber length and the aspect ratio of fibers while maintaining the same volume fraction also improved both the flexural capacity and toughness of the beam. Furthermore, the beam's peak load was severely reduced using large fiber diameters, especially for fiber diameters of 0.9 mm and 1.0 mm. However, the beam heat to induce prestressing by the shape memory effect showed a higher peak load than that of the non-heated case. However, the heated beams showed a lower toughness capacity and disappearance of the initial crack point compared to the non-heated beam. Thus, the mesoscale finite element method can intensely examine the effects of the geometry of fibers on flexural behavior with acceptable results with low cost and time consumption compared to experimental tests.