In a common salt-in-polymer electrolyte, a polymer which has polar groups in the molecular chain is necessary because the polar groups dissolve lithium salt and coordinate cations. Based on the above point of view, polystyrene [PS] that has nonpolar groups is not suitable for the polymer matrix. However, in this PS-based composite polymer-in-salt system, the transport of cations is not by segmental motion but by ion-hopping through a lithium percolation path made of high content lithium salt. Moreover, Al2O3 can dissolve salt, instead of polar groups of polymer matrix, by the Lewis acid-base interactions between the surface group of Al2O3 and salt. Notably, the maximum enhancement of ionic conductivity is found in acidic Al2O3 compared with neutral and basic Al2O3 arising from the increase of free ion fraction by dissociation of salt. It was revealed that PS-Al2O3 composite solid polymer electrolyte containing 70 wt.% salt and 10 wt.% acidic Al2O3 showed the highest ionic conductivity of 9.78 × 10-5 Scm-1 at room temperature.
Polyurethane foam manufacturing depends on its materials and processes. A polyol that contains primary alcohol is very reactive with isocyanate. Sometimes, this may cause unexpected problems. In this study, a semi-rigid polyurethane foam was fabricated; however, its collapse occurred. The cellulose nanofiber was fabricated to solve this problem, and a weight ratio of 0.25, 0.5, 1, and 3% (based on total parts per weight of polyols) of the nanofiber was added to the polyurethane foams. The effect of the cellulose nanofiber on the polyurethane foams’ rheological, chemical, morphological, thermal, and anti-collapse performances was analyzed. The rheological analysis showed that 3 wt% of the cellulose nanofiber was unsuitable because of the aggregation of the filler. It was observed that the addition of the cellulose nanofiber showed the improved hydrogen bonding of the urethane linkage, even if it was not chemically reacted with the isocyanate groups. Moreover, due to the nucleating effect of the cellulose nanofiber, the average cell area of the produced foams decreased according to the amount of the cellulose nanofiber present, and the average cell area especially was reduced about five times when it contained 1 wt% more of the cellulose nanofiber than the neat foam. Although the thermal stability declined slightly, the glass transition temperature shifted from 25.8 °C to 37.6, 38.2, and 40.1 °C by when the cellulose nanofiber increased. Furthermore, the shrinkage ratio after 14 days from the foaming (%shrinkage) of the polyurethane foams decreased 15.4 times for the 1 wt% cellulose nanofiber polyurethane composite.
Multi-functional magnetite–polysilsesquioxane (PSSQ) hybrid nanoparticles were synthesised in a one-pot approach using ferrous and ferric chlorides and various silane monomers by coprecipitation followed by a surface grafting method. The functional groups, surface properties, and thermal stability of the materials were analyzed using a range of characterisation techniques. Furthermore, the functional magnetic hybrid nanoparticles were used for the adsorption of heavy metal ions. The results suggest that the magnetic PSSQ hybrid nanoparticles have excellent adsorption and selectivity behavior for iron (Fe3+) and some heavy metal ions as individual ions or in mixtures of metal ions. The adsorption kinetics highlighted the excellent adsorption behavior of the functionalised magnetic PSSQ hybrid nanoparticles. On the other hand, the adsorption behavior depends on the type of functional groups present in the materials. These promising and highly desirable magnetic hybrid materials can be used in a wide range of applications.
Herein, we propose a facile method for the synthesis of functionalised mesoporous silica nanoparticles (MSN) via the polymerisation of N-isopropylacrylamide (NIPAM) monomer with vinyl functional mesoporous silica nanoparticles (VMSN). The structural and functional properties of the materials are analysed using various characterisation techniques. Additionally, a transparent hydrophobic glass substrate is fabricated by dispersing a certain amount of the synthesised nanoparticles in ethyl acetate (EA) followed by spin-coating on a glass substrate and drying overnight at 80 °C. In summary, the functionalised mesoporous materials can be used for multiple applications such as the preparation of stable hydrophobic, transparent, and temperature-sensitive surfaces, as well as for the adsorption of Rhodamine B dye.