Against the background of low global carbonization, blast furnace ironmaking technology with coking puts huge amounts of pressure on the global steel industry to save energy and reduce emissions due to its high pollution levels and high energy consumption. Bath smelting reduction technology is globally favored and studied by metallurgists as a non-blast furnace ironmaking technology that directly reduces iron ore into liquid metal without using coke as the raw material. The smelting reduction reaction of iron ore, which is the core reaction of the process, is greatly significant to its productivity and energy saving. Therefore, this paper focuses on the behavior and mechanism of iron ore’s smelting reduction. This work focuses on three key aspects of smelting reduction, namely, the thermal decomposition characteristics of iron ore during the smelting reduction, the smelting reduction mechanism of iron-ore particles, and the smelting reduction mechanism of FeO-bearing slag. The experimental study methods, reaction mechanisms, influencing factors, and kinetic behavior of the three are highlighted. In this work, the reaction mechanism of thermal iron-ore decomposition, iron-ore particle smelting reduction, and FeO-bearing slag smelting reduction on the three reactions were observed, providing a theoretical basis for how to select and optimize raw materials for the bath smelting reduction process. Moreover, the kinetic study clarifies the limiting steps of the reactions and provides guidance for an improvement in the reaction rate. However, certain blank points in previous studies need to be further explored, such as the differences in the research results of same factor, the large variation in reaction activation energy, and the coupling mechanism and inter-relatedness of the three key aspects’ reactions with each other.
The phenomenon of cracking and deterioration of iron ore particles is a widespread scientific problem in the field of mineral processing and metallurgy. In this paper, the thermal decomposition properties of iron ore were investigated by a non-isothermal method using thermogravimetric equipment, and the crack evolution behavior of iron ore within Fe-C melt was investigated experimentally, by scanning electron microscopy and Micro-CT. The results show that the start decomposition temperature of #2 iron ore is 292.7 °C, which is 37.3 °C higher compared to that of #1 iron ore, because of its smaller pores and the difficulty of water vapor diffusion. The initial decomposition of iron ore is the decomposition goethite to form water vapor, and as heat transfer continues, hematite particles break into smaller particles and decompose to form Fe3O4. During the smelting reduction process, the Crack index (CI) of #1 iron ore was 5.50% at 4 s, and the CI index increased to 23.54% when time was extended to 16 s, and the internal evolved from locally interconnected holes to cracked structure. The iron ore maintains a relatively intact form during reduction within the Fe-C melt, and interfacial reduction reaction is dominant in the later stage.
Hydrogen-rich blast furnace ironmaking is an important low-carbon technology to reduce CO2 emissions of steel industry, and its effect on softening-melting performance has a great influence on blast furnace ironmaking. In this paper, the softening-melting properties of basic pellets with hydrogen-rich based on high pellets ratio ironmaking were studied. The microstructure evolution and softening-melting mechanism of pellets during the process were investigated. The results show that when the hydrogen concentration increases from 0% to 12%, the initial softening temperature (T10) decreases from 1209°C to 1197°C, the melting starting temperature (Ts) and dripping temperature (Td) increase respectively, which means bottom the cohesive zone descends. S-value decreases from 458.55kPa·°C to 293.33kPa·°C. In hydrogen-rich condition, hydrogen will not gather on the surface of pellets like CO to form a dense iron shell. More FeO is produced on the surface and inside of pellets, which forms the low-melting-point slag phase with gangue and reduces the initial softening temperature. And after entering the melting stage, the FeO produced inside decreases, resulting a high melting point of slag, So, the dripping temperature increases from 1412°C to 1458°C.
Hydrogen-enriched blast furnace ironmaking has emerged as one of the pivotal technologies for decarbonizing the integrated steelmaking route. To further investigate the hydrogen-rich reduction behavior of iron-bearing materials in blast furnaces, this study systematically examines the hydrogen-rich reduction reaction of basic pellets through interruption experiments combined with microstructural characterization and phase analysis. Experimental results demonstrate that the basic pellets achieved a 79.7% reduction degree in CO-N2 atmosphere, which increased significantly to 93.7% with 16vol% H2, confirming hydrogen's remarkable enhancement effect on the reduction index of basic pellets. In the initial of reduction, CO accumulates on the surface of pellets, resulting metal iron on the surface, while the interior is the initial Fe2O3 state. But hydrogen enhances the internal reduction degree. Hydrogen-rich promotes more thorough reduction of internal microparticles within basic pellets. XRD results indicate that in the later stage of CO reduction, the FeO peak of pellets is stronger. XRD fitting analysis demonstrate that FeO phase is 37.85% after 180min reduction, and the FeO phase of pellets reduced by reducing gas concluding 8vol% H2 accounts for 14.79wt%.