A novel and environmentally friendly recycling approach for carbon-fiber-reinforced plastics (CFRP) was studied using not only nitric acid (HNO3) but also our chosen alkaline, sodium hydrogen carbonate (NaHCO3). The CFRP specimen was first immersed into 8 M HNO3 at 80 °C for 8 h, and then into 0.1 M NaHCO3 at 80 °C for 15 min to obtain resin-free recycled carbon fiber (rCFs). Using this new recycling method, it was shown that the recycling time was reduced to 8.3 h, whereas it originally took 24 h, as reported previously. It was shown that immersing the CFRP specimen into NaHCO3 caused a transesterification reaction with the remaining resin residue on the CF surface, which led to dissolving the resin into the NaHCO3 aqueous solution all at once. Additionally, NaHCO3 produced carbon dioxide gas while reacting with the resin residue; the CO2 gas physically helped removing the resin from the CF’s surface. Moreover, evaluating the physical properties of the rCFs demonstrated an improvement in fiber strength and adhesiveness to resin. Therefore, this recycling method was shown to be effective in recovering high-quality rCFs in a relatively short recycling period.
To effectively reuse a large amount of Carbon Fiber Reinforced Plastics (CFRP) waste, the carbon fibers should be able to be recovered without degrading their quality. In this report, we developed a new approach to recover carbon fibers from CFRPs with improved physical properties compared to virgin carbon fibers with an environmentally friendly recycling method using nitric acid. Following the decomposition of the CFRP waste in nitric acid at 80 °C, both recycled carbon fibers and decomposed resin were recovered. The obtained recycled carbon fibers showed 1.4 times higher tensile strength and 2.2 times higher interfacial shear strength to resin compared to virgin carbon fibers. TEM-EDX analysis showed a decrease in the abundance of voids existing in the carbon fiber surface layer and new polar functional groups caused by nitric acid existing inside the voids, leading to increased tensile strength. Furthermore, XPS analysis showed that the interfacial shear strength improved due to the formation of new polar functional groups due to nitric acid. The possibility of applying recycled carbon fibers to CFRP products was shown by elucidating the mechanism that expressed its physical properties during the recycling process, leading to a novel approach to realizing closed-loop recycling.
Functionalization of graphite is crucial for efficient and effective exfoliation to graphene. When negative charges are fixed to the edges of natural graphite, the resulting anionic graphite shows negative charging in a polar solvent. This enhanced negative charging is assumed to contribute the exfoliation of graphite during liquid-phase exfoliation (LPE). In this study, we prepared large anionic graphite flakes (~10 μm) by salt-assisted ball milling, as well as natural graphite flakes of the same size for comparison. During the LPE process, centrifugation speed and solvent type have dominant effects on graphene concentration and quality (e.g., size and thickness), so we investigated these factors for anionic graphite flakes in detail. The anionic graphite showed higher exfoliation efficiency in every type of solvent (isopropanol, methyl ethyl ketone, acetone, and water-based cosolvent) compared with the natural graphite. Monolayer graphene, with an average size of 80–200 nm, was obtained with relatively high yield (>10%) at only 3 min of sonication. The small size of graphene was due to edge fragmentation during the LPE process. The recyclability of the sediment and the characterization of the exfoliated powders for anionic graphene were also investigated.