In order to study the mechanical properties of rubber concrete (RC) with different rubber particle sizes after dry–wet cycles in a sulfate environment, apparent morphology analysis, mass loss analysis, relative dynamic elastic modulus analysis, compressive strength loss analysis, internal microscopic characteristics and deterioration degree analysis of ordinary concrete (NC) and rubber concrete after dry–wet cycles were compared and analyzed. The results show that with the increase in the number of dry–wet cycles, the surface caves of rubber concrete increase, the internal microcracks develop and penetrate, and the macroscopic strength increases first and then decreases significantly. The high elasticity of rubber effectively improves the expansion force caused by sulfate attack and the dry–wet cycle. The deterioration degree of RC in each dry–wet cycle stage is obviously better than that of NC. When the rubber particle size is 0.85 mm, the performance of the sample is the best. After 120 days of dry–wet cycle, the compressive strength is reduced by 37.4%, and the compressive strength of concrete with a rubber particle size of 0.85 mm is reduced by 11.2%. After cyclic loading, the deterioration degree of concrete is 5.1% lower than that of ordinary concrete.
In order to study the mechanical properties of rice husk ash–rubber–fiber concrete (RRFC) under hygrothermal environment, the optimal group was selected by orthogonal test. The mass loss, relative dynamic elastic modulus analysis, strength analysis, degradation degree analysis after cyclic loading and internal microstructure analysis of the optimal group of RRFC samples after dry–wet cycles under different environments and temperatures were compared and analyzed. The results show that the large specific surface area of rice husk ash optimizes the particle size distribution of RRFC specimens, reacts to form C-S-H gel, enhances the compactness of concrete, and forms a dense structure as a whole. The presence of rubber particles and PVA fibers effectively improves the mechanical properties and fatigue resistance of RRFC. The comprehensive mechanical properties of RRFC with rubber particle size of 1–3 mm, PVA fiber content of 1.2 kg·m−3 and rice husk ash content of 15% are the best. The compressive strength of the specimens after dry–wet cycles in different environments generally increased first and then decreased, reaching a peak at the seventh dry–wet cycle, and the compressive strength of the specimens under chloride salt solution decreased more than that under clear water solution. Thes provided new concrete materials for the construction of highways and tunnels in coastal areas. Under the premise of ensuring the strength and durability of concrete, it is of great practical significance to explore new roads for energy conservation and emission reduction.
With the depletion of shallow resources, deep resource mining has become a trend. However, the high temperature and complex stress environment in deep mines make resource extraction extremely challenging. This paper developed a thermal insulation grouting material made of glazed hollow beads, sodium silicate, and cement and tested the compressive strength, gelation time, and stone rate under various curing days in light of the issue of high temperature heat damage in high ground temperature mines and the impact of mining on roadway grouting bolt support. Fatigue strength, fatigue deformation, load-residual strain, energy evolution and microscopic features were studied and analyzed in relation to the damage law of graded cyclic loading and unloading under the number of varying cycles. The findings demonstrate that cyclic loading and unloading strength is lower than uniaxial compressive strength. The fatigue strength is significantly decreased when the number of cycles reaches its limit. Residual strain is less sensitive to changes in stress than load strain. The fitting correlation coefficients of total output energy and elastic energy are higher than 0.71.