Friction stir welding (FSW) is an effective solid-state joining process that has the potential to overcome common problems correlated with conventional fusion welding processes. FSW is used for the joining of metallic materials, in particular Al alloys (non-heat-treatable and heat-treatable). The heat produced by the friction between the rotating tool and the workpiece material generates a softened region near the FSW tool. Although the heat input plays a crucial role in producing a defect-free weld metal, it is a serious concern in the FSW of work-hardened non-heat-treatable Al alloys. In this group of alloys, the mechanical properties, including hardness, tensile properties, and fatigue life, are adversely affected by the softening effect because of grain growth and reduced dislocation density. Considering this challenge, work-hardened Al alloys have been limited in their industrial use, which includes aerospace, shipbuilding, automotive, and railway industries. The current comprehensive review presents the various approaches of available studies for improving the quality of FSW joints and expanding their use. First, the optimization of welding parameters, including the tool rotational and traverse speeds, tool design, plunge depth, and the tilt angle is discussed. Second, the incorporation of reinforcement particles and then underwater FSW are stated as other effective strategies to strengthen the joint. Finally, some supplementary techniques containing surface modification, bobbin tool FSW, copper backing, and double-sided FSW in relation to strain-hardened Al alloys are considered.
In this study, friction stir welding (FSW) was employed to join AA3003-H18 sheets by incorporating in situ Al-Cu intermetallic compounds within the stir zone. The FSW process was carried out under three distinct conditions: (I) without applying powder, (II) by introducing Cu powder, and (III) by incorporating Cu-Al mixed powder (50 vol.% Cu, 50 vol.% Al). The powder was embedded into the gap between two sheets. Subsequently, two-pass FSW, involving both forward and backward movements, was conducted with a rotational speed of 1200 rpm and traverse speed of 100 mm/min across all three experimental conditions. In the second and third conditions, the formation of in situ intermetallic compounds occurred through a solid-state reaction between Cu particles and Al within the stir zone. Examination of the stir zone through optical and electron microscopic studies revealed that the utilization of Cu-Al mixed powder resulted in finer and more uniformly distributed Cu clusters and Al-Cu intermetallics than samples welded with Cu powder alone. Notably, the stir zone of samples incorporating Cu-Al mixed powder exhibited finely dispersed, completely gray Al-Cu intermetallic particles, whereas those with only Cu powder displayed predominantly coarse core-shell particles in the microstructure. The introduction of Cu-Al mixed powder during FSW resulted in a stir zone with an average hardness of 74 HB, showing a 14% increase compared to the cases where Cu powder alone was added (65 HB). Tensile tests, conducted in both transverse and longitudinal directions on the FSWed samples, did not exhibit a consistent trend across the three mentioned conditions. Transverse tensile strength consistently ranged between 107 and 110 MPa, with joint efficiency varying from 52% to 54%. However, the longitudinal tensile strength of the joint with added Cu-Al mixed powder (158 MPa) surpassed those welded with Cu powder alone (134 MPa).