Yottha Srithep

Dr. Yottha Srithep

manufacturing engineering, Mahasarakham University, Maha Sarakham, Thailand
orcid

Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 June 2017 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
DPD Pholharn
D Pholharn
YSYottha Srithep
Yottha Srithep
JMJ Morris
J Morris
We studied the effect of several aliphatic alcohols, including1-dodecanol, 1-octanol and methanol, as initiators on synthesis of poly(L-lactide) (PLLA) by ring opening polymerization. The reaction starts with L-lactide monomer and uses stannous octoate as catalyst. Fourier transform infrared spectroscopy and X-ray diffraction analysis verified that PLLAs were produced successfully. Weight, number average molecular weight and polydispersity index of PLLAs were measured by gel permeation chromatography. The PLLA initiated by methanol (PLLA-Meth) presented the highest molecular weight and yield percent. From differential scanning calorimetry, PLLA-Meth showed the highest melting temperature at ~167°C, crystallization temperature at 110°C and degree of crystallinity 80%. The thermal stability was assessed by thermogravimetric analysis: this confirmed that PLLA-Meth was superior with the highest degradation temperature compared to PLLA initiated by other initiators. We concluded that methanol was the most appropriate initiator for PLLA synthesis by ring opening polymerization.

19 April 2017 in e-Polymers
Verified
Journal Article
Open access
PDF file
YSYottha Srithep
Yottha Srithep
DPDutchanee Pholharn
Dutchanee Pholharn
Poly( l -lactide) (PLLA)/poly( d -lactide) (50/50) with plasticizer contents ranging from 2% to 16% w/w were prepared by melt blending using an internal mixer. Wide-angle X-ray diffraction, Fourier transform infrared spectroscopy and differential scanning calorimetry results confirmed that complete stereocomplex polylactide crystallites without any homocrystallites were produced. Compared to neat PLLA, the melting temperature of the stereocomplex polylactide and its plasticized samples was approximately 55°C higher. Higher plasticizer contents decreased glass transition temperature of the stereocomplex, which implied higher flexibility and enhanced the crystallization rate. However, the plasticizer in the stereocomplex reduced the thermal stability.

1 January 2021 in Journal of Renewable Materials
Verified
Journal Article
Open access
YSYottha Srithep
Yottha Srithep
OVOnpreeya Veang-In
Onpreeya Veang-In
DPDutchanee Pholharn
Dutchanee Pholharn
LTLih-Sheng Turng
Lih-Sheng Turng
JMJohn Morris
John Morris
A low-molecular-weight polylactide-poly(butylene succinate) (PLA-PBS) copolymer was synthesized and incorporated into polylactide (PLA) as a novel toughening agent by solvent casting. The copolymer had the same chemical structure and function as PLA and it was used as a plasticizer to PLA. The copolymer was blended with PLA at a weight ratio from 2 to 10 wt%. Phase separation between PLA and PLA-PBS was not observed from their scanning electron microscopy (SEM) images and the crystal structure of PLA almost remained unchanged based on the X-ray diffraction (XRD) measurement. The melt flow index (MFI) of the blends was higher as the amount of PLA-PBS increased, indicating that the block copolymer did improve the mobility of the PLA chains. Moreover, tensile tests revealed that PLA with greater PLA-PBS copolymer exhibited higher elongation at break and it reached the maximum at 8 wt% of PLA-PBS in PLA, which was around 6 times higher than that of pure PLA. Furthermore, the glass transition temperature, measured by differential scanning calorimetry (DSC), markedly decreased with an increasing amount of the copolymer as it decreased from 61.2°C for pure PLA to 41.3°C when it was blended with 10 wt% PLA-PBS copolymer. Therefore, the PLA-PBS copolymer was shown to be a promising plasticizer for fully biobased and toughened PLA.

29 May 2014 in Journal of Polymer Engineering
Verified
Journal Article
Closed access
YSYottha Srithep
Yottha Srithep
WRWuttipong Rungseesantivanon
Wuttipong Rungseesantivanon
BHBongkot Hararak
Bongkot Hararak
KSKrisda Suchiva
Krisda Suchiva
Currently, use of poly(lactic acid) (PLA) is limited for commercial applications because it has a low heat resistance. In this research, an increase of over 40°C heat distortion temperature (HDT) of PLA alloy was obtained by blending PLA with polycarbonate (PC) and a chain extender (CE). Molecular weight, thermal, mechanical and morphological properties of PLA and PC blend with different CE contents were investigated. Gel permeation chromatography (GPC) results showed that some PLA-PC copolymers were produced and the compatibility of the PLA phase and in the PC phase was improved via the chain extension reaction. In addition, the reaction induced by CE also affected the crystallization behaviors of PLA, as observed from differential scanning calorimetry (DSC) results and the enthalpy of melting of PLA decreased with increasing CE content. The combined effects of the CE increasing molecular weight, improving compatibility and limiting the crystallization behavior of PLA/PC alloy greatly improved the HDT.

26 April 2023 in Polymers
Verified
Journal Article
Open access
PDF file
YSYottha Srithep
Yottha Srithep
DPDutchanee Pholharn
Dutchanee Pholharn
PWPatnarin Worajittiphon
Patnarin Worajittiphon
KSKeartisak Sriprateep
Keartisak Sriprateep
OVOnpreeya Veang-In
Onpreeya Veang-In
JMJohn Morris
John Morris
The high cost, low heat resistance, and brittleness of poly(L-lactide) (PLLA) is a significant drawback that inhibits its diffusion into many industrial applications. These weaknesses were solved by forming a polylactide stereocomplex (ST) and blending it with thermoplastic starch (TPS). We blended poly (L-lactide)(PLLA), up to 30% thermoplastic starch, and a chain extender (2%) in an internal mixer, which was then hand-mixed with poly (D-lactide)(PDLA) and injection molded to form specimens, in order to study mechanical, thermal, and crystallization behavior. Differential scanning calorimetry (DSC) and wide-angle X-ray diffraction (XRD) demonstrated that the stereocomplex structures were still formed despite the added TPS and showed melting points ~55 °C higher than neat PLLA. Furthermore, stereocomplex crystallinity decreased with the increased TPS content. Dynamic mechanical analysis revealed that ST improved PLLA heat resistance, and tensile testing suggested that the TPS improved the elongation-at-break of ST. Moreover, the chain extender reduced the degradation of ST/TPS blends and generally improved ST/TPS composites’ mechanical properties.

1 June 2017 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
YSYottha Srithep
Yottha Srithep
DPD Pholharn
D Pholharn
ADA Dassakorn
A Dassakorn
JMJ Morris
J Morris
Poly(ethylene terephthalate) (PET) based thermoplastics are common, particularly in packaging. Due to both thermal and hydrolytic degradation, recycled PET (rPET) shows poor mechanical properties. The effect of adding 30% polycarbonate (PC) and chain extender (CE) on mechanical, thermal and morphological properties was investigated. rPET with PC and CE was melt blended in a single screw extruder, which was then tensile test specimens were formed by injection molding rPET and PC compatibility was improved via chain extending reactions which in turn improved the rPET and PC blend mechanical properties. With the addition of 30%PC the tensile modulus of rPET increased by 18% and it increased by 223% when 2%CE was added to rPET and 30%PC blends. Also, the CE reaction affected crystallization, monitored by differential scanning calorimetry: the melting enthalpy ofblends was lowered by increased CE content.