CFRP structures are often exposed to humid environment resulting in water absorption and causing property degradation. Water swelling and its effect on tensile, compressive, and flexural properties were investigated according to ASTM standards. Fracture modes were evaluated by analyzing micrographs of fracture areas. The specimens were cut from twill wave CFRP composite plates fabricated using a vacuum infusion technique. Some of them were immersed in water prior to being mechanically tested. It was found that tensile strength, as well as compressive, and flexural strength and moduli decreased due to water swelling, but fracture strain was found to increase due to water swelling. The most severely affected by water swelling is flexural strength (decreased by 25.72%), and the least is compressive modulus (decreased by 1.89%). Tensile specimens underwent fibre breakage followed by matrix cracking, compressive and flexural specimens showed fibre buckling followed by kinking and crushing where flexural specimens failed in their compressive side. In conclusion, water absorption has a bad impact on the composite strength.
26 February 2021 in Eastern-European Journal of Enterprise Technologies
Heat exchangers are important equipment for the process of placing heat. The most widely used type of heat exchanger is shell and tube. This type is widely used because of its simple and easy design. Design of shell and tube heat exchangers is done by the side or shell variations to get the desired performance. Therefore, research is conducted to study the effect of tube thickness on heat transfer, pressure drop, and stress that occurs in the shell and tube heat exchanger so that the optimal tube thickness is obtained. In this research, the activities carried out are the design of heat exchangers for the production of oxygen with a capacity of 30 tons/day. The standard used in this study is the 9th edition heat exchanger design guidance document compiled by the Tubular Exchanger Manufacturer Association (TEMA). Analysis of the tube thickness effect on heat transfer, pressure drop, and stress was carried out using the SimScale platform. The effect of variations in tube thickness on heat transfer is that the thicker the tube, the lower the heat transfer effectiveness. The highest value of the heat exchanger effectiveness is 0.969 at the tube thickness variation of 0.5 mm. The lowest value of the heat exchanger effectiveness is 0.931 at the tube thickness variation of 1.5 mm. The effect of variations in tube thickness on pressure drop is that the thicker the tube, the higher the pressure drop. The highest value of pressure drop is in the variation in tube thickness of 1.5 mm, 321 Pa. The lowest value of drop pressure is in the variation of 0.5 mm tube thickness, which is 203 Pa. The thickness of the tube also increases the maximum stress on the components of the shell, head, tubesheet, baffle, and saddle, but the value is fluctuating
This research aims to investigate the carbon fiber reinforced polymer (CFRP) when subjected to tensile, bending, and compression. Half of the specimens are also subjected to water to find out how water influences. The CFRP is created using a combination of carbon fiber layers and epoxy resin Bisphenol A Epichlorohydrin with hardener and is formed using the vacuum infusion method. From the water absorption test, it was found that the average weight gain of the specimens was 2.9% and the lowest value was at 0.6%, it was concluded that the increase in wet specimen weight was not too significant and water absorption tended to be slow. Mechanical testing ob-tained the highest average tensile stress, bending stress, compressive stress, and modulus of elasticity of 195 MPa, 295 MPa, 96 MPa, and 8914 MPa were from dry specimens while the lowest average values were 146 MPa, 286 MPa, 81 MPa, and 6160 MPa from wet specimens. The results of micro-photo observations on the tensile test fracture show that the specimen has a XGM fracture character with delamination and splitting fractures happening in multiple areas. In the bending test, the specimens experienced buckling fracture due to the fiber breaking and the inability of the matrix to withstand the additional stress. Shear fracture happened during the compressive test. In conclusion, water absorption has a bad impact towards the composite strength.
29 February 2024 in Journal of Applied Research and Technology
Hybrid ratio effect on flexural properties of sugar palm/E-glass fiber hybrid-reinforced polyester composites has been investigated. Before being embedded, the sugar palm fiber was taken off from its original mesh, washed, alkali-treated, and chopped into ~10 mm long. The specimens were cut from composite plates having different hybrid ratios, fabricated using cold pressed technique. The total fiber volume fraction was kept at ~0.21, where four hybrid ratios, and two span-to-depth ratios were used. The E-glass was arranged unidirectionally and placed right on the surface of a bottom mold and wetted using the matrix, and the SPF was then evenly poured on the wet E-glass arrangement in randomly oriented pattern. Specimen preparation and testing were carried out according to the ASTM D790 standard, where the E-glass sides were placed in tension sides of the beams. It was found that flexural strength, and strain at maximum stress significantly increase with the increase of hybrid ratio.
1 February 2020 in Journal of Physics: Conference Series
The effect of temperature and time duration of degumming process on tensile properties of Pandanus Tectorius fibers has just been studied. While degumming temperature and soaking time for alkali treatment were kept constant at 80 °C and 2 hours, respectively, degumming time was varied at 1, 2, 3 and 4 hours, and sodium hydroxide solution content was varied at 2.5 and 5 wt%. A bundle of fiber was placed in an O-shape cardboard holder for being tensile tested until fracture occurred. Cross sectional areas and fracture modes of representative fibers were captured under optical microscope. Whilst the cross section image areas were then measured by means of an open source software, the imageJ, the fracture images were closely evaluated to determine their respective fracture modes. The result showed that tensile strength, tensile failure strain and elastic modulus increase with the increase of degumming time up to 3 hours, then decrease for 4 hours degumming time. The highest values were found being 614.5 MPa, 0.11 mm/mm and 1.07 GPa, respectively.