Electromagnetic properties of polymer composites strongly depend on the loading amount and the completeness of the filler’s dispersive structure. Improving the compatibility of single-walled carbon nanotubes (SWCNTs) with isobutylene butyl rubber (IIR) is a good solution to mitigate aggregation. The change in configuration of poly-oxyethylene octyl phenol ether (OP-10) was induced using water as the exposed hydrophilic groups linking with water molecules. The SWCNT and IIR/SWCNT composites were then prepared via wetly-melt mixing at a relatively high temperature to remove water, and they were then mixed with other agents after vacuum drying and cured. The SWCNTs were dispersed uniformly to form a good network for a lower percolation threshold of the wave-absorbing property to 2 phr from 8 phr. With 8 phr SWCNTs, the tensile strength of the material improved significantly from 7.1 MPa to 15.1 MPa, and the total electromagnetic shielding effectiveness of the material was enhanced to 23.8 dB, a 3-fold increase compared to the melt-mixed material. It was demonstrated that water-induced modification achieved good dispersion of SWCNTs for electromagnetic shielding enhancement while maintaining a wide damping temperature range from −55 °C to 40 °C with a damping factor over 0.2.
Electromagnetic (EM) pollution becomes more penetrating in daily life and work due to more convenience provided by multi-electrical devices, as does secondary pollution caused by electromagnetic reflection. EM wave absorption material with less reflection is a good solution to absorb unavoidable EM radiation or reduce it from the source. Filled with two-dimensional Ti3SiC2MXenes, silicone rubber (SR)composite demonstrated a good electromagnetic shielding effectiveness of 20 dB in the X band by melt-mixing processes for good conductivity of more than 10−3 S/cm and displayed dielectric properties and a low magnetic permeability; however, the reflection loss was only −4 dB. By the combination of one-dimensional highly electric conductive multi-walled carbon nanotubes (HEMWCNTs) and MXenes, the composites achieved the transformation from electromagnetic inflection to an excellent absorbing performance to reach a minimum reflection loss of −30.19 dB due to electric conductivity of above 10−4 S/cm, a higher dielectric constant, and more loss in both dielectric and magnetic properties. Ni-added multi-walled carbon nanotubes were not able to achieve the transformation. The as-prepared SR/HEMWCNT/MXene composites have potential application prospects in protective layers, which can be used for electromagnetic wave absorption, electromagnetic interference suppression of devices, and stealth of the equipment.
29 April 2008 in Journal of Chemical Crystallography