Molasses wastewater (MWW) is characterized by high organic loading and a recalcitrant dark brown color. A study was carried out to determine the photocatalytic efficiency of TiO2–ZnO nanohybrid supported onto activated carbon (AC) for the remediation of MWW. Immobilization of ZnO onto TiO2 formed TiO2–ZnO, which was then supported onto AC forming TiO2–ZnO–AC composite. X-ray diffraction (XRD), scanning electron (SEM), energy-dispersive X-ray (EDX) and Fourier transform infrared (FTIR) spectroscopies, and transmission electron (TEM) microscopy revealed the successful hybridization of TiO2 and ZnO, and the subsequent support of the hybrid onto AC. Photoluminescence (PL) spectroscopy further revealed a restrained electron-hole pair recombination resulting from both the successful formation of a heterojunction, and the introduction of electron accepting AC support. Photodegradation process was monitored by color and total organic carbon (TOC) reductions. It was observed that TiO2–ZnO (ratio 3:1) supported onto AC (30% loading) had a higher adsorptive capacity and catalytic activity than bare TiO2–ZnO resulting in a 14% increment in overall color reduction. UV-photodegradation was found to be very effective for color as compared to TOC reduction, with 96% and 9% reductions, respectively, after 1 hour of irradiation. A pH of 5 was found to be optimum for photodegradation.
13 October 2017 in Journal of Environmental Science and Health, Part A
This study evaluated the photocatalytic activity of polyaniline (PANI)-capped titanium dioxide and zinc oxide (TiO2/ZnO) hybrid, for the degradation of P-Cresol. The hybrid was synthesized by precipitating ZnO on the surface of commercial TiO2. An “in situ” chemical oxidative polymerization method was used to prepare the PANI capped hybrid (TiO2/ZnO/PANI). The photocatalysts were characterized by powder X-ray diffraction (XRD), a Brunauer Emmett Teller (BET) analyzer, Fourier-transform infrared (FTIR) and photoluminescence spectroscopies, high resolution-transmission electron microscopy (HR-TEM) and thermogravimetric analysis (TGA). During photodegradation under ultraviolet (UV) irradiation, ZnO, TiO2, TiO2/ZnO hybrid and TiO2/ZnO/PANI composite had P-Cresol removal of 43%, 50%, 61% and 99%, respectively. The higher activity of the TiO2/ZnO hybrid as compared to TiO2 and ZnO was attributed to a reduced electron–hole pair recombination. The recombination was further significantly reduced upon introduction of PANI; hence, the highest activity observed with TiO2/ZnO/PANI. The initial reaction rate constant for TiO2/ZnO/PANI (0.9679 min−1) was more than twice compared to that for TiO2/ZnO hybrid (0.1259 min−1). A synergistic effect between PANI and TiO2/ZnO resulted in a highly efficient charge separation caused by the transfer of photogenerated holes from the hybrid to highest occupied molecular orbitals (HOMO) of PANI. The best TiO2/ZnO/PANI (PANI to TiO2/ZnO) ratio observed was 0.5:2 for the photodegradation of P-Cresol. Total organic carbon (TOC) analysis indicated a 97.4% mineralization of P-Cresol with PANI/TiO2/ZnO.
Effective treatment of waste streams such as municipal waste-activated sludge (WAS) presents an opportunity for energy and nutrient recovery, water reclamation, and mitigation of climate change. WAS is a waste product of the activated sludge treatment (AST) process widely used for municipal wastewater. Currently, WAS treatment and disposal account for up to 50% of the total operation cost and 40% of the total greenhouse gas emissions from wastewater treatment plants. Anaerobic digestion (AD) is usually preferred for WAS treatment since it is more economical compared to other existing technologies. The decomposition of sludge during AD releases nutrients, which are then discharged in the anaerobic effluent, polluting recipient water bodies and increasing the nutrient burden. The nutrients, mainly nitrogen (N), phosphorus (P), and potassium (K), can be crystallised into struvite (magnesium ammonium phosphate, NH4MgPO4.6H2O) with numerous agricultural applications as fertilisers. The present review focusses on struvite recovery from anaerobically digested WAS and its potential application for crop production. Graphical Abstract
10 March 2017 in Journal of Environmental Science and Health, Part A
A hybrid photo-catalyst, TiO2-ZnO, was synthesized by immobilizing ZnO on commercial TiO2 (aeroxide P25). Activated carbon (AC) was subsequently used to support the hybrid, thus forming a TiO2-ZnO/AC composite catalyst. Fourier transform infrared (FTIR) analysis and scanning electron microscopy integrated with energy-dispersive X-ray spectroscopy (SEM-EDX) investigations revealed successful catalyst synthesis. Optical properties of the hybrid determined from photoluminescence (PL) and Ultraviolet-visible (UV-vis) spectroscopy confirmed a restrained recombination of electron-hole pairs and reduced energy band gap due to a successful heterojunction formation. The prepared catalysts were used to photodecolorise vinasse in a 12-W UVC batch photoreactor. TiO2-ZnO had improved photocatalytic activity compared with TiO2 and ZnO separately. On supporting the hybrid onto AC, both adsorption and photocatalytic activities were further enhanced with improved overall color removal of 86% from 68%. Photodecolorisation followed the pseudo-first-order reaction model with the rate constant ( ) observed decreasing from 0.0701 to 0.0436 min−1 on increasing the initial concentration from 5,000 to 14,000 ppm. The UV process was found to be 33-fold less energy intensive for color reduction as compared to total organic carbon (TOC) reduction. Formation of nitrates during the photodecolorisation process was attributed to the mineralization of nitrogen heteroatoms in the color-causing melanoidin compounds.
In this study, the ozonolysis of real anaerobically digested distillery wastewater (DWW) was carried out. The effect of operating parameters, such as pH, initial concentration, and ozone dosage, on the efficiency of ozone utilization, color removal, and sludge solubilization was studied. The highest ozone utilization of 99% was observed at the highest initial concentration (COD of 3000 mg/L) and lowest ozone flowrate (22.5 mg O3/L/min), but with a very low color reduction of 20%, after 60 minutes of ozonolysis. To achieve a higher color reduction >80% and at ozone utilization >95%, the DWW had to be diluted twice (COD 1500 mg/L), and the flowrate doubled to 45 mg O3/L/min. The reduction in color signified the oxidation of the color causing biorecalcitrant aromatic melanoidin compounds. This was confirmed by the 47% reduction in ultraviolet absorbance at 254 nm indicating the breakdown of the complex aromatic compounds into low molecular weight organics. Moreover, increases in average oxidation state from −0.6 to −0.2 suggested a decline in aromaticity and formation of easily biodegradable aliphatic compounds. The ozonolysis process was found to follow the first-order reaction kinetic model with the highest rate constant of 0.0326 min−1 obtained. A reduction in suspended COD by 88% indicated solubilization of the sludge contained in the effluent.