MnBi alloy was prepared using arc melting, and was then heated at various temperatures and times. The alloy was ball milled for various lengths of time, following a heat treatment at 573 k for 20 h. The effects of the heat treatment and the ball milling on the magnetic performances of the material were investigated by analyzing the phases, the particle sizes, and the grain sizes. Results showed that the mass percentage of the LTP MnBi phase increased as the heat treatment time increased. The mass percentage initially increased and then decreased as the heat treatment temperature increased. The saturation magnetization increased quickly as the mass percentage of the LTP MnBi increased following the heat treatment. The value rose as high as 71.39 emu/g at 573 K for 30 h. The magnetization decreased, due to the decomposition of MnBi phases after ball milling. The coercivity increased simultaneously, due to the grain refinement, the presence of stresses, defects, and an amorphous phase. This value was improved from 0.09 KOe to 14.65 KOe after ball milling for 24 h.
Al-TiCN composites were fabricated by spark plasma sintering (SPS). The effect of TiCN content (0, 1, 3, 5, 7 and 10 wt.%) on the microstructure and mechanical properties of as-SPSed composites were investigated. Results show that TiCN particles are uniformly dispersed in Al powder except Al-10 wt.% TiCN composite, which contains excessive TiCN particles results in agglomeration of TiCN particles. Besides, the hardness of composites increases with increasing TiCN content. The maximum hardness of composites is 35.2 HV, which is 14% higher than that of the Al matrix. Moreover, Al-7 wt.% TiCN composite exhibits the most excellent comprehensive properties with its compressive strength at 45% strain higher by 11% as compared to the Al matrix. The superior mechanical properties of Al-TiCN composites were mainly attributed to Orowan strengthening due to TiCN particles.
17 November 2023 in Journal of Materials Engineering and Performance