Undesired solid precipitation in coal slag at high temperatures can cause serious blockages, or even the shutdown of coal gasifiers, due to a rapid increase in slag viscosity. In this study, the solid precipitation behaviors of coal slag from different primary phases and under different atmospheres were both experimentally and theoretically investigated. Our results demonstrated that the viscosity of the coal slag in the primary phase of mullite was strongly influenced by the atmosphere at a typical tapping temperature of 1300 °C because of the high content of network formers. The viscosity of the partially crystallized slag was significantly affected by solid precipitation behavior. Iron was converted to magnetite and hematite in air and was reduced to metallic iron under a reducing atmosphere. Increasing CaO content improved both the iron reduction reaction and the slag crystallization behavior. Anorthite precipitation was largely inhibited under a mild reducing atmosphere, leading to a large difference in the viscosity of coal slag under different atmospheres. In contrast, the viscosity of the coal slag in the primary phase of mullite was slightly influenced by the atmosphere due to the weak crystallization tendency of mullite, as well as its high slag viscosity.
The entrained-flow gasification technology is an efficient way to achieve the large-scale utilization of coal. In the entrained-flow gasification process, the Na from coal is readily released to the gas phase and then condensed at the surface of the coal gasification fly ash (CGFA), improving the sintering of the CGFA deposited on the surface of the syngas cooler and causing serious ash deposition problem. However, the effect of the NaCl on the CGFA remains unexplored. In this study, the effect of the NaCl on the sintering behavior of CGFA was investigated via an in-situ heating stage and compressive strength analysis, and the sintering mechanism was revealed by a novel coupled kinetic-thermodynamic phase analysis method. Results demonstrated that the sintering process of CGFA was divided into the solid sintering stage, plateau stage, and the liquid sintering stage. The NaCl increased the shrinkage rate of CGFA and improved the solid precipitation at a relatively low temperature. Under the isothermal sintering condition, the plateau stage occurred in advance in the presence of NaCl. The NaCl addition benefited the CGFA densification process at a low dosage and resulted in high compressive strength. A moderate adding content of NaCl accelerated the solid precipitation reaction and the viscous flow of CGFA. However, the compressive strength of CGFA was decreased at a high NaCl content for the disrupt of the aluminosilicate network structure, although the albite crystallization was enhanced. Results of this study is significant for understanding the CGFA deposition mechanism contributed by the Na from coal.