The practical application of rechargeable aqueous zinc-ion batteries (ZIBs) has been severely hindered by detrimental dendrite growth, uncontrollable hydrogen evolution, and unfavorable side reactions occurring at the Zn metal anode. Here, we applied a Prussian blue analogue (PBA) material K2Zn3(Fe(CN)6)2 as an artificial solid electrolyte interphase (SEI), by which the plentiful -C≡N- ligands at the surface and the large channels in the open framework structure can operate as a highly zincophilic moderator and ion sieve, inducing fast and uniform nucleation and deposition of Zn. Additionally, the dense interface effectively prevents water molecules from approaching the Zn surface, thereby inhibiting the hydrogen-evolution-resultant side reactions and corrosion. The highly reversible Zn plating/stripping is evidenced by an elevated Coulombic efficiency of 99.87% over 600 cycles in a Zn/Cu cell and a prolonged lifetime of 860 h at 5 mA cm−2, 2 mAh cm−2 in a Zn/Zn symmetric cell. Furthermore, the PBA-coated Zn anode ensures the excellent rate and cycling performance of an α-MnO2/Zn full cell. This work provides a simple and effective solution for the improvement of the Zn anode, advancing the commercialization of aqueous ZIBs.
Aqueous zinc-ion batteries (AZIBs) show enormous potential as a large-scale energy storage technique. However, the growth of Zn dendrites and serious side reactions occurring at the Zn anode hinder the practical application of AZIBs. For the first time, we reported a fluorine-containing surfactant, i.e., potassium perfluoro-1-butanesulfonate (PPFBS), as an additive to the 2 M ZnSO4 electrolyte. Benefitting from its hydrophilic sulfonate anion and hydrophobic long fluorocarbon chain, PPFBS can promote the uniform distribution of Zn2+ flux at the anode/electrolyte interface, allowing the Zn/Zn cell to cycle for 2200 h. Furthermore, PPFBS could inhibit side reactions due to the existence of the perfluorobutyl sulfonate (C4F9SO3−) adsorption layer and the presence of C4F9SO3− in the solvation structure of Zn2+. The former can reduce the amount of H2O molecules and SO42− in contact with the Zn anode and C4F9SO3− entering the Zn2+-solvation structure by replacing SO42−. The Zn/Cu cell exhibits a superior average CE of 99.47% over 500 cycles. When coupled with the V2O5 cathode, the full cell shows impressive cycle stability. This work provides a simple, effective, and economical solution to the common issues of the Zn anode.
13 June 2023 in The Journal of Physical Chemistry C
Ether-based electrolytes have attracted considerable interest in the development of potassium-ion batteries (PIBs) owing to their superior compatibility with potassium metal anodes. Nevertheless, their inherently limited electrochemical stability windows, particularly with respect to inadequate oxidative stability, pose significant challenges for the practical implementation of high-voltage cathodes exceeding 4 V. Traditional ether electrolytes tend to undergo rapid decomposition at elevated potentials, leading to the deterioration of the cathode-electrolyte interphase and severe capacity degradation. In this study, we present a solvation chemistry engineering approach by incorporating Bis(2-fluoroethyl) carbonate (BFC) into a 1,3-dioxane electrolyte. The addition of BFC modifies the solvation sheath structure, enhances the desolvation kinetics of potassium ions (K + ), and simultaneously broadens the electrochemical stability window. As a result, the optimized electrolyte facilitates stable cycling of high-voltage cathodes operating at approximately 4.5 V in PIBs, achieving a remarkable capacity retention of 92.2% after 1800 cycles under high current densities, alongside an outstanding Coulombic efficiency of 99.95%. This work establishes a framework for the deliberate manipulation of solvation chemistry in the design of high-voltage electrolytes and provides a viable strategy to overcome the voltage limitations inherent to ether-based electrolyte systems.