The 2000 series aluminium alloys are qualified for widespread use in lightweight structures, but solidification cracking during fusion welding has been a long-standing issue. Here, we create a zirconium (Zr)-core-aluminium (Al)-shell wire (ZCASW) and employ the oscillating laser-arc hybrid welding technique to control solidification during welding, and ultimately achieve reliable and crack-free welding of 2024 aluminium alloy. We select Zr wires with an ideal lattice match to Al based on crystallographic information and wind them by the Al wires with similar chemical components to the parent material. Crack-free, equiaxed (where the length, width and height of the grains are roughly equal), fine-grained microstructures are acquired, thereby considerably increasing the tensile strength over that of conventional fusion welding joints, and even comparable to that of friction stir welding joints. This work has important engineering application value in welding of high-strength aluminum alloys.
Brittle intermetallic compounds, formed during the welding process of titanium/aluminum (Ti/Al), lead to a significant reduction in joint mechanical properties. The purpose of this study is to mitigate the formation of brittle phases during the laser welding of dissimilar Ti/Al metals, thereby enhancing the mechanical properties of the joints. In this investigation, an innovative approach is adopted, utilizing Nb foil as an interlayer to effectively minimize the formation of brittle intermetallic phases during dissimilar welding. A comprehensive analysis of the microstructure of the transition layer was conducted using material characterization methods, including scanning electron microscope equipped with an energy dispersive X-ray spectrometer. The mechanical performance of the welded joints was assessed using tensile testing. The results indicate that the effective welding width and joint penetration depth at the joint interface were reduced in Ti/Al dissimilar metals when Nb was added as an intermediate layer, under the same welding process parameters, when compared to unalloyed weld seams. Furthermore, the utilization of a 0.05 mm Nb foil as the intermediate layer results in a significant 25% increase in the average shear strength compared to the other condition, with the average shear strength of the joint reaching its peak value at 192 N/mm. The unalloyed Ti/Al weld joint usually fractured along the melting zone, displaying complete brittle fracture characteristics. After Nb microalloying, the joint typically fractures along the transition zone and interface, exhibiting both cleavage and ductile fracture characteristics, indicating the combination of a brittle and toughness fracture. This study provides experimental evidence and new insights for welding Ti/Al composite structures, with significant theoretical and practical applications.