High mechanical residues at/after elevated temperatures are basic prerequisites for the engineering applications of carbon fiber reinforced polymer (CFRP) composites in special fields like aerospace. In this study, phthalonitrile (PNP) copolymers based on hydroxyl compounds of BP monomer, PEP and BZCN resin were designed and their curing behavior and processability were investigated for realizing the corresponding CFRP composites. High temperature mechanical performances of PNP/hydroxyl compound/CF composites under instantaneous and non-instantaneous states are systematically assessed. At 300 °C, PNP/hydroxyl compounds/CF composite showed a retention rate of tensile, compressive, flexural strength and flexural modulus higher than 35%, 95%, 80% and 90%, respectively. After 300 °C/50 h thermal aging, their flexural properties show no obvious attenuation. Even after being aged at 350 °C for 50 h, the residue of flexural modulus is above 90% while that of flexural strength is over 60%. The mass residue of PNP/hydroxyl compounds/CF composites were all higher than 98% and 90% after aging at 300 °C and 350 °C for 50 h. PNP/hydroxyl compounds/CF composites, with the excellent comprehensive mechanical properties, can be used as high performance engineering materials.
Shock-induced opacity in Gd3Ga5O12 (GGG) single crystals is investigated by transmission/emission measurements at 16 wavelengths (400–800 nm), as well as complementary particle velocity measurements at 1550 nm, in the pressure range of 47–211 GPa. Optical transmission spectra through the shocked samples are measured with a in-situ, shock-generated light source, and the resultant extinction coefficients of different wavelengths and shock pressures obtained. As shock strength increases, the optical opacity of the shocked GGG increases and peaks at 75 GPa (the transparent–opaque transition), drops at 75–100 GPa (the opaque–transparent transition), and then increases again. The transparency recovery coincides with a solid–solid phase transition. The microstructure changes associated with the solid–solid phase transition and plastic deformation most likely cause the loss and recovery of transparency. GGG can be useful as a high pressure window for laser velocimetry (1550 nm) or optical pyrometry (400–800 nm) in the ranges of 100–140 GPa and 80–120 GPa, respectively.