Direct laser irradiation of sputter deposited Al/Pt nanolaminate multilayers results in rapid local heating and exothermic mixing of reactant layers. Milli- and microsecond pulsed laser irradiation under certain test conditions leads to single-point ignition of rapid, self-propagating, formation reactions. Multilayers having bilayer thicknesses of 328 nm, 164 nm, and 65 nm are characterized by their ignition onset times and temperatures. Smaller bilayer thickness multilayers require less laser intensity for ignition compared with larger bilayer designs (when utilizing a particular pulse duration). The relationship between laser intensity and ignition onset time is used to calibrate an activation energy for ignition within a finite element reactive heat transport model. The local heating rate is varied from 104 K/s to 106 K/s by selecting a laser intensity. Kissinger analysis was performed on the heating rate-dependent ignition temperatures measured with high speed pyrometry to experimentally determine an activation energy in the foils of (6.2 ± 1.6 × 104 J/mole atoms). This value is then compared to an activation energy produced from model fits to an ignition onset time of 7.2 × 104 J/mole atoms.
Nanothermite NiO–Al is a promising material system for low gas emission heat sources; yet, its reactive properties are highly dependent on material processing conditions. In the current study, sputter deposition is used to fabricate highly controlled nanolaminates comprised of alternating NiO and Al layers. Films having an overall stoichiometry of 2Al to 3NiO were produced with different bilayer thicknesses to investigate how ignition and self-sustained, high temperature reactions vary with changes to nanometer-scale periodicity and preheat conditions. Ignition studies were carried out with both hot plate and laser irradiation and compared to slow heating studies in hot-stage x-ray diffraction. Ignition behavior has bilayer thickness and heating rate dependencies. The 2Al/3NiO with λ ≤ 300 nm ignited via solid/solid diffusion mixing (activation energy, Ea = 49 ± 3 kJ/mole). Multilayers having λ ≥ 500 nm required a more favorable mixing kinetics of solid/liquid dissolution into molten Al (Ea = 30 ± 4 kJ/mole). This solid/liquid dissolution Ea is a factor of 5 lower than that of the previously reported powder compacts due to the elimination of a passivating Al oxide layer present on the powder. The reactant mixing mechanism between 300 and 500 nm bilayer thicknesses was dependent on the ignition source's heating rate. The self-propagating reaction velocities of 2Al/3NiO multilayers varied from 0.4 to 2.5 m/s. Pre-heating nanolaminates to temperatures below the onset reaction temperatures associated with forming intermediate nickel aluminides at multilayer interfaces led to increased propagation velocities, whereas pre-heating samples above the onset temperatures inhibited subsequent attempts at laser ignition.
The interaction between multiple intense ultrashort laser pulses and solids is known to produce a regular nanoscale surface corrugation. A coupled mechanism has been identified that operates in a specific range of fluences in GaAs that exhibits transient loss of the imaginary part of the dielectric function and Χ2, which produces a unique corrugation known as high spatial frequency laser induced periodic surface structures (HSFL). The final structures have 180 nm periods, and their alignment perpendicular to the laser polarization is first observed in an intermediate morphology with correlation distances of 150 ± 40 nm. Quantum molecular dynamics simulations suggest that HSFL self-assembly is initiated when the intense laser field softens the interatomic binding potential, which leads to an ultrafast generation of point defects. The morphological evolution begins as self-interstitial diffusion, driven by stress relaxation, to the surface producing 1–2 nm tall islands. An ab initio calculation of excited electron concentration combined with a Drude-Lorentz model of the excited GaAs dielectric function is used to determine that the conditions for SPP coupling at HSFL formation fluences are both satisfied and occur at wavelengths that are imprinted into the observed surface morphologies. The evolution of these morphologies is explained as the interplay between surface plasmon polaritons that localize defect generation within the structures present on the previous laser exposure and stress relaxation driven defect diffusion.