This study utilized bismaleimide (BMI) resin, reinforced with introduced ether bonds, as a binding matrix, in combination with silicon carbide (SiC), for the fabrication of composite materials. A thorough investigation was conducted to assess the influence of diverse processing parameters on the mechanical properties and high-temperature thermo-oxidative stability of these composites. Experimental results indicate a notable improvement in the mechanical properties of the composites upon the incorporation of ether bonds, in contrast to their unmodified counterparts. The variation in performance among composites with different ratios and molding densities is apparent. Within a certain range, an increase in resin content and molding density is correlated with improved bending strength in the composites. With a resin content of 27.5 vol% and a molding density of 2.31 g/cm3, the composite achieved a maximum flexural strength of 109.52 MPa, representing a 24% increase compared to its pre-modification state. Even after exposure to high-temperature heat treatment, the composites displayed commendable mechanical properties compared to their pre-ether bond modification counterparts, maintaining 74.5% of the strength of the untreated composites at 300 °C. The scanning electron microscopy (SEM) microstructures of composite materials correlate remarkably well with their mechanical properties.
Currently, the sol-gel technique is employed in the synthesis of high-performance vitrified bonds; however, its application in the fabrication of stacked abrasives has been minimally explored. Furthermore, the methods utilized in the production of abrasive particles for stacked abrasives are technically challenging and incur high costs, which hinders their actual industrial application. Consequently, this study utilizes the sol-gel approach to synthesize a Na2O-B2O3-SiO2 ternary system vitrified bond powder and employs a molding and crushing method, which offers a lower technological barrier and reduced preparation costs, for the production of abrasive particles subsequently fabricating corundum stacked abrasives. Upon setting the binder composition to a molar ratio of n(SiO2):n(B2O3):n(Na2O) = 65:23:12, it was observed that the crystallization within the glass matrix was minimized and the optimal sintering temperature for the synthesized laminate abrasive to be sustained at 820 °C. At the aforementioned temperature, the binder melt is capable of flowing uniformly amongst the abrasive granules, thereby ensuring a robust encapsulation of the particles. The average single particle compressive strength of the prepared corundum stacked abrasive with a grain size of forty mesh can reach the highest of all composition points at 28.56 N and the average single particle compressive strength of the prepared diamond stacked abrasive is 28.14 N.
In this research, we report the synthesis of Si–TmC–B/PCD composites using Si, B, and transition metal carbide particles (TmC) as binders at high pressure and high temperature (HPHT method, 5.5 GPa and 1450 °C). The microstructure, elemental distribution, phase composition, thermal stability, and mechanical properties of PCD composites were systematically investigated. The Si–B/PCD sample is thermally stable in air at 919 °C. The initial oxidation temperature of the PCD sample with ZrC particles is as high as 976 °C, and it also has a maximum flexural strength of 762.2 MPa, and the highest fracture toughness of 8.0 MPa·m1/2.