Zhenbo Zuo

Dr. Zhenbo Zuo


Research Focus & Metrics

Academic Career Length

4Years (2023-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
7 February 2024 in Materials
Verified
Journal Article
Open access
PDF file
ZZZhenbo Zuo
Zhenbo Zuo
Rui HuRui Hu
Rui Hu
QWQ.X Wang
Q.X Wang
ZGZitong Gao
Zitong Gao
Xian LuoXian Luo
Xian Luo
SLShaoqiang Li
Shaoqiang Li
Research on how thermal exposure affects the microstructure and mechanical properties of the Ti–48Al–3Nb–1.5Ta (at. %) alloy, which is prepared via powder hot isostatic pressing (P–HIP), is essential since this low-density alloy shows promise for use in high-temperature applications, particularly for aero-engines, which require long-term stable service. In this study, a P–HIP Ti–48Al–3Nb–1.5Ta (at. %) alloy was exposed to high temperatures for long durations. The phase, microstructure and mechanical properties of the P–HIP Ti–48Al–3Nb–1.5Ta alloy after thermal exposure under different conditions were analyzed using XRD, SEM, EBSD, EPMA, TEM, nanomechanical testing and tensile testing. The surface scale is composed of oxides and nitrides, primarily Al2O3, TiO2, and TiN, among which Al2O3 is preferentially generated and then covered by rapidly growing TiO2 as the thermal exposure duration increases. The nitrides appear later than the oxides and exist between the oxides and the substrate. With increasing exposure temperature and duration, the surface scale becomes more continuous, TiO2 particles grow larger, and the oxide layer thickens or even falls off. The addition of Ta and Nb can improve the oxidation resistance because Ta5+ and Nb5+ replace Ti4+ in the rutile lattice and weaken O diffusion. Compared with the P–HIP Ti–48Al–3Nb–1.5Ta alloy, after thermal exposure, the grain size does not increase significantly, and the γ phase increases slightly (by less than 3%) with the decomposition of the α2 phase. With increasing thermal exposure duration, the γ phase exhibits discontinuous coarsening (DC). Compared with the P–HIP Ti–48Al–3Nb–1.5Ta alloy, the hardness increases by about 2 GPa, the tensile strength increases by more than 50 MPa, and the fracture strain decreases by about 0.1% after thermal exposure. When the depth extends from the edge of the thermally exposed specimens, the hardness decreases overall.

7 July 2023 in Metals
Verified
Journal Article
Open access
PDF file
ZZZhenbo Zuo
Zhenbo Zuo
Rui HuRui Hu
Rui Hu
Xian LuoXian Luo
Xian Luo
HTHongkui Tang
Hongkui Tang
ZZZhen Zhu
Zhen Zhu
SLShaoqiang Li
Shaoqiang Li
In this study, Ti-48Al-3Nb-1.5Ta powders were manufactured from cast bars by the supreme-speed plasma rotating electrode process (SS-PREP) and used to prepare hot isostatically pressed (HIPed) material at 1050–1260 °C with 150 MPa for 4 h. The phase, microstructure and mechanical performance were analyzed by XRD, SEM, electrical universal material testing machine and other methods. The results revealed that the phase constitution changed from γ phase to α2 phase and then to γ phase with the material changing from as-cast to powders and then to as-HIPed. Compared with the as-cast material, the grain size and element segregation were significantly reduced for both powders and as-HIPed. When the hot isostatic pressing (HIP) temperature was low, the genetic characteristics of the powder microstructure were evident. With the HIP temperature increasing, the homogeneity of the composition and microstructure increased, and the prior particle boundaries (PPBs) gradually disappeared. The elastic moduli of powder and as-HIPed were superior to those of as-cast, which increased with the HIP temperature increasing. The hardness of as-HIPed was lower than that of the powder. The compressive strength, compressive strain, bending strength, and tensile strength of as-HIPed were higher than those of as-cast. With an increase in the HIP temperature, the compressive strength decreased gradually, and the compressive strain first decreased and then increased.

20 September 2025 in Metals
Verified
Journal Article
Open access
PDF file
ZZZhenbo Zuo
Zhenbo Zuo
Rui HuRui Hu
Rui Hu
SLShaoqiang Li
Shaoqiang Li
CLChengpeng Liu
Chengpeng Liu
QWQ.X Wang
Q.X Wang
LKLu Kang
Lu Kang
In this study, various characterization techniques were utilized to investigate the effects of heat treatments on the microstructure and mechanical properties of Ti-48Al-3Nb-1.5Ta (at. %) alloy prepared by the supreme-speed plasma rotating electrode process and hot isostatic pressing. By comparing the microstructures of the alloy under different heat treatments conditions, it was found that the nearly lamellar structure with a size of about 145 μm is formed by a simple heat treatment (1400 °C/10 min, FC to 1300 °C, AC, 850 °C/3 h/FC). Under this heat treatment condition, the alloy exhibited satisfied mechanical properties, with a tensile fracture strain of 1.2% at room temperature and a tensile fracture strain of 7.5% at 750 °C. No fracture occurred after 225 h when creeping at 750 °C/250 MPa. Ta inhibited the growth of lamellae and the expansion of pores, thereby improving creep performance. In summary, the TiAl alloy with satisfied performance was obtained through a simple heat treatment process, which provides a significant idea for engineering application.