Montmorillonite, the major clay mineral in the tailings of weathered crust elution-deposited rare earth ores, was modified as an excellent adsorbent to enrich rare earth ions from solutions. It was demonstrated that 5% H2SO4 could be used as a modifier to effectively enhance the adsorption capacity of montmorillonite after modifying for 3 h with a liquid:solid ratio of 40:1 at 90 °C. A superior modified montmorillonite over montmorillonite on adsorption performance was analyzed by the XRD, FT-IR, SEM, and BET (Specific Surface Area and Pore Diameter Analysis). The adsorption behaviors of La3+ and Y3+ on modified montmorillonite were fitted well with the Langmuir isotherm model and their saturated adsorption capacities were 0.178 mmol/g to La3+ and 0.182 mmol/g to Y3+, respectively. Furthermore, (NH4)2SO4 as a common leaching agent in weathered crust elution-deposited rare earth ores, were successfully used as the eluent to recover the adsorbed rare earth ions.
In situ leaching of weathered crust elution-deposited rare earth ore usually uses ammonium sulfate as the leaching agent, which poses challenges such as low mass transfer efficiency, high consumption of the leaching agent and long leaching periods. In order to intensify the leaching process of rare earth elements and reduce the impurity of leaching accompanying rare earth, ammonium sulfate and ammonium formate were mixed as a novel compound leaching agent to treat weathered crust elution-deposited rare earth ore. The effects of ammonium formate concentration, liquid/solid ratio, leaching agent pH and leaching temperature on the leaching process of rare earth (RE) and aluminum (Al) were investigated and evaluated using the chromatographic plate theory. Results showed that ammonium formate could effectively enhance the mass transfer efficiency of rare earth and significantly inhibit the mass transfer efficiency of aluminum. Leaching agent pH has a greater impact on the mass transfer efficiency of aluminum. A higher leaching temperature could enhance the mass transfer efficiency of rare earth and aluminum by providing a driving force to overcome the resistance of diffusion. The optimum conditions for leaching rare earth and aluminum are 0.1 mol/L ammonium sulfate compounded with 0.032 mol/L ammonium formate, pH 4–8 of the leaching agent, 0.8:1 liquid:solid (mL/g) ratio and room temperature. Under this condition, the mass transfer efficiency of rare earth was improved, and the mass transfer efficiency of aluminum was significantly inhibited.