Stainless steel (SS316L) and titanium alloy (Ti6Al4V) exhibit suitable properties for biomedical applications; however, the tribocorrosion of these materials, which is associated with metallosis, is still a significant concern. This work investigates the effectiveness of DLC smoothing coatings applied to the metals to reduce tribocorrosion and improve cell viability. The study was motivated by many reports of metallosis caused by metal debris in the soft tissues of the body. DLC coatings were produced using the plasma-enhanced chemical vapor deposition (PECVD) technique. The cytotoxicity, genotoxicity, and cell viability of metallic samples with and without DLC coatings were analyzed, considering the chemical composition of the coating and metallic components. The results show that the DLC coatings presented suitable interaction properties and no cytotoxicity or genotoxicity when exposed to the cellular environment, compared with the control group (p < 0.0001). They also demonstrated cell viability, low friction representing a reduction of 80%, and hardness 23–26 GPa, making them ideal for use on fixed implants. It is necessary to control the thickness and roughness of the coating to avoid pinholes and increase the corrosion protection of implants. These DLC coatings with low friction coefficients could facilitate the fixation of implantable pins and screws, including Kirschner wires.
Stainless steel 316L (SS316L) and titanium-alloy Ti6AL4V exhibit properties for bio-medical applications; however their tribocorrosion associated with metallosis is still a major concern. Therefore smoothing DLC coatings aiming for the improvement of tri-bocorrosion and cell viability of stainless steel 316L (SS316L) and titanium-alloy Ti6AL4V with and without DLC coatings were compared. The motivation was due to many papers detailing metallosis caused by metal debris in the body's soft tissues. Nowadays, metallosis is responsible for almost of prosthesis replacement surgeries. DLC coatings were produced using the Plasma Enhanced Chemical Vapor Deposition (PECVD) technique; acetylene gas was used as a carbon precursor, and silane gas produced an amorphous silicon interface between the DLC coating and metal substrate. A combined setup of techniques thoroughly evaluated the coatings considering chemical composition, coatings adhesion at a metallic substrate, scratch resistance, and tribocorrosion susceptibility. The cytotoxicity and genotoxicity of metallic samples with and without DLC coatings were analyzed, considering cell viability and its correlation with coatings’ chemical composition
This study presents an innovative dual-layer coating approach integrating titanium dioxide (TiO2) onto diamond-like carbon (DLC)-coated 316L stainless steel. The combination of PECVD-deposited DLC and ALD-deposited TiO2 aims to preserve the inherent tribological properties of DLC while mitigating UV-induced degradation. By leveraging the ability of TiO2 to absorb, reflect, and scatter UV light, this dual-layer strategy significantly enhances the durability of DLC coatings in radiation-prone environments. The effects of accelerated aging through UV exposure on DLC and DLC/TiO2 films were evaluated using an Accelerated Weathering Tester. Comprehensive analyses were conducted to assess the structural and mechanical properties before and after UV exposure, including Raman spectroscopy, profilometry, SEM, EDS, nanoindentation, and tribometry. The results demonstrate that the TiO2 layer effectively mitigates UV-induced damage, preserving the DLC film’s integrity and tribological performance even after 408 h of UV aging. Specifically, the DLC/TiO2 coatings maintained lower roughness, higher hardness, and better adhesion than DLC-only coatings under identical conditions. This research significantly advances protective coating technology by enhancing the durability and performance of DLC films, particularly in aerospace and other demanding industries where exposure to UV radiation is a critical concern.