Nd-Fe-B-based permanent magnets are widely used for energy conversion applications. However, their usage at elevated temperatures is difficult due to the relatively low coercivity (Hc) with respect to the anisotropy field (HA) of the Nd2Fe14B compound, which is typically 0.2HA. In this work, we found that the coercivity of an (Nd0.8Dy0.2)-Fe-B sintered magnet could reach 0.4HA, which was twice as high as the Hc/HA of its Dy-free counterpart. Detailed microstructural characterizations, density functional theory and micromagnetic simulations showed that the large value of coercivity, Hc = 0.4HA, originated not only from the enhanced HA of the main phase (intrinsic factor) but also from the reduced magnetization of the thin intergranular phase (extrinsic factor). The latter was attributed to the dissolution of 4 at.% Dy in the intergranular phase that anti-ferromagnetically coupled with Fe. The reduction in the magnetization of the intergranular phase resulted in a change in the angular dependence of coercivity from the Kondorsky type for the Dy-free magnet to the Stoner–Wohlfarth-like shape for the Dy-containing magnet, indicating that the typical pinning-controlled coercivity mechanism began to show nucleation features as the magnetization of the intergranular phase was reduced by Dy substitution.
24 August 2021 in The Journal of Physical Chemistry C
Magnetic cooling, harnessing the temperature change in matter when exposed to a magnetic field, presents an energy‐efficient and climate‐friendly alternative to traditional vapor‐compression refrigeration systems, with a significantly lower global warming potential. The advancement of this technology would be accelerated if irreversible losses arising from hysteresis in magnetocaloric materials are minimized. Despite extensive efforts to manipulate crystal lattice constants at the unit‐cell level, mitigating hysteresis often compromises cooling performance. Herein, we address this persistent challenge by forming Sn(Ge) 3 −Sn(Ge) 3 bonds within the unit cell of the Gd 5 Ge 4 compound. This approach enables an energetically favorable phase transition, leading to the elimination of thermal hysteresis. Consequently, we achieve a synergistic improvement of two key magnetocaloric figures of merit: a larger magnetic entropy change and a twofold increase in the reversible adiabatic temperature change (from 3.8 to 8 K) in the Gd 5 Sn 2 Ge 2 compound. Such synergies can be extended over a wide temperature range of 40–160 K. This study demonstrates a paradigm shift in mastering hysteresis toward simultaneously achieving exceptional magnetocaloric metrics and opens up promising avenues for gas liquefaction applications in the longstanding pursuit of sustainable energy solutions.
30 July 2025 in Science and Technology of Advanced Materials
Magnetic cooling technology, based on the magnetocaloric effect (MCE), offers an energy-efficient and eco-friendly alternative to conventional gas compression, but is often hindered by large magnetic hysteresis, which limits cyclic performance. In this study, we show that the hysteresis of La0.7Ce0.3(Fe,Si)₁₃ hydrides – a promising material for room-temperature refrigeration – can be significantly reduced by refining the microstructure of the precursor alloy. Substituting Ce for La in (La0.7Ce0.3)(Fe,Si)13Hx increases hysteresis losses from 12.3 J/kg to 34 J/kg. However, preparing the precursor alloy using the melt-spinning technique can almost eliminate this hysteresis. Lorentz transmission electron microscopy (Lorentz-TEM) shows that phase transition nucleation preferentially occurs at the grain boundaries. The hydrides prepared from melt-spun ribbons exhibit a much larger volume fraction of grain boundaries due to finer grains, providing a higher density of nucleation sites. This reduces the energy barrier for the phase transition and weakens the magneto-structural phase transition, as confirmed by in-situ X-ray diffraction patterns. Consequently, the reduced phase transition energy barrier leads to significantly lower hysteresis in melt-spun hydrides samples. These findings demonstrate the potential of microstructure engineering to reduce hysteresis in (La,Ce)(Fe,Si)13Hₓ materials for room-temperature magnetocaloric applications.
To develop low-cost, high-performance light rare earth element (LRE)-substituted Nd–Fe–B permanent magnets, we systematically studied the effect of substituting Nd with 20% light rare earth elements (LRE = Ce, Y, and La) on the hard magnetic properties of (Nd0.8LRE0.2)–Fe–B hot-deformed magnets. The (Nd0.8Ce0.2)2Fe14B magnet showed a coercivity of μ0Hc = 1.41 T, which is comparable to that of an LRE-free magnet. Y substitution was found to decrease μ0Hc and μ0Mr to 1.22 and 1.32 T, respectively, as was expected from the intrinsic properties of (Nd0.8Y0.2)2Fe14B. Unlike our expectation, the thermal stability of coercivity is not degraded by the Y substitution, demonstrating its potential for elevated temperature applications. With La substitution, coercivity is substantially degraded to 0.67 T because of the low intrinsic properties and the lack of the intergranular phase. The Y and Ce co-substituted (Nd0.8Ce0.1Y0.1)2Fe14B hot-deformed magnets showed better thermal stability of coercivity compared to the (Nd0.8Ce0.2)2Fe14B sample.