Objective. The aim of this study was to evaluate alternative methods for the disinfection of denture-based materials.Material and Methods. Two different denture-based materials were included in the study. Before microbial test, the surface roughness of the acrylic resins was evaluated. Then, the specimens were divided into 8 experimental groups, according to microorganism considered and disinfection methods used. The specimens were contaminated in vitro by standardized suspensions ofCandida albicansATCC#90028 andCandida albicansoral isolate. The following test agents were tested: sodium hypochlorite (NaOCl 1%), microwave (MW) energy, ultraviolet (UV) light, mouthwash containing propolis (MCP), Corega Tabs, 50% and 100% white vinegar. After the disinfection procedure, the number of remaining microbial cells was evaluated in CFU/mL. Kruskal-Wallis, ANOVA, and Dunn’s test were used for multiple comparisons. Mann WhitneyUtest was used to compare the surface roughness.Results. Statistically significant differencewas found between autopolymerised and heat-cured acrylic resins. The autopolymerised acrylic resin surfaces were rougher than surfaces of heat-cured acrylic resin. The most effective disinfection method was 100% white vinegar for tested microorganisms and both acrylic resins.Conclusion. This study showed that white vinegar 100% was the most effective method for tested microorganisms. This agent is cost-effective and easy to access and thus may be appropriate for household use.
1 January 2014 in The Journal of Advanced Prosthodontics
Purpose: The objective of this in vitro study was to investigate and compare two-body wear of hybrid, microhybrid, and nanohybrid direct and indirect composite resins. Materials and methods: A pin-on-disc wear device was used to study the effects of the water on two-body wear rate of two microhybrid composites (Solidex® and Dialog®), a nanohybrid composite (Grandio®SO), and three direct composite resins: a hybrid composite (Herculite Classic™), a submicron hybrid composite (Charisma®), and a nanohybrid composite (Tetric® N-Ceram). For testing, 12 specimens of each material with 6.5 mm diameter and 4 mm height were made and half of the specimens were stored in the distilled water for 1 week at 37℃. In order to evaluate the wear rate of samples, a normal load of 15 N was applied to specimen’s surface. The 6.5 mm diameter composite sample held to pin holder and AISI 316 L stainless steel was employed as the disc. The following experimental parameters were kept constant for all tests: sliding velocity = 0.6 m/s, temperature 25 ± 3℃, 1.2 Hz, and 10,000 cycles. One-way Analysis of Variance (ANOVA) and post hoc Tukey’s test were performed to compare the wear rate of resin composites. Results: Ranking of wear rate (most to least) without water exposure was as follows: Dialog>Solidex>Charisma>GrandioSO>Tetric Ceram=Herculite. No significant difference in wear was observed between GrandioSO, Tetric N-Ceram, and Herculite Classic, with and without water exposure (p > .05, respectively). Conclusions: The nanohybrid resins—regardless of indirect or direct use—showed significantly less abrasive wear than the microhybrid resins.
When preparing prosthetic restorations, dentists always try to create restorations functionally ideal while not compromising on esthetics. The factors that make a restoration successful include how well they fit both internally and marginally, their ability to withstand punishment without breaking, and their visual appeal. Imperfect marginal adaptation can lead to unpleasant and unwanted side effects such as plaque accumulation, marginal discoloration, microleakage, carious and endodontic lesions, and periodontal disease. If there is a gap between the crown and the prepared tooth, this can result in the dissolution of the luting material. If the fit of the restoration and the thickness of the cement are designed to be favorable, the cement is not dissolved and the abutment tooth is prevented from secondary caries. The marginal fit of the restorations is considerably affected by the materials and techniques used when making dental crowns. This chapter contains reviews on marginal fitting and caries.