Orawan Khamman

Dr. Orawan Khamman

orcid

Research Focus & Metrics

Academic Career Length

21Years (2006-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
21 February 2006 in Materials Letters
Verified
Journal Article
Closed access
ARApinpus Rujiwatra
Apinpus Rujiwatra
STSaowalak Tapala
Saowalak Tapala
SLSanchai Luachan
Sanchai Luachan
OKOrawan Khamman
Orawan Khamman
SASupon Ananta
Supon Ananta

2 January 2024 in Journal of Asian Ceramic Societies
Verified
Journal Article
Open access
PWPimpilai Wannasut
Pimpilai Wannasut
MPMethee Promsawat
Methee Promsawat
AWAnucha Watcharapasorn
Anucha Watcharapasorn
SESukum Eitssayeam
Sukum Eitssayeam
SASupon Ananta
Supon Ananta
OKOrawan Khamman
Orawan Khamman

24 July 2023 in Materials
Verified
Journal Article
Open access
PDF file
MKManlika Kamnoy
Manlika Kamnoy
KPKamonpan Pengpat
Kamonpan Pengpat
TTTawee Tunkasiri
Tawee Tunkasiri
OKOrawan Khamman
Orawan Khamman
UIUraiwan Intatha
Uraiwan Intatha
SESukum Eitssayeam
Sukum Eitssayeam
Photoluminescent (PL) layers and electroluminescent (EL) systems have gained significant attention for their applications in constructing flat panels, screen monitors, and lighting systems. In this study, we present a groundbreaking approach to fabricating temperature sensors using barium-calcium zirconium titanate (BCZT) with thermo-optic properties, leading to the development of opto-thermal sensors for electric vehicle battery packs. We prepared zinc sulfide (ZnS) fluorescent films on BCZT ceramics, specifically two optimal compositions, BCZT0.85 (Ba0.85Ca0.15Zr0.1Ti0.9O3) and BCZT0.9 (Ba0.9Ca0.1Zr0.1Ti0.9O3), via the solid-state reaction method for the dielectric layer. The BCZT powders were calcined at varying temperatures (1200 and 1250 °C) and dwell times (2 and 4 h). The resulting phase formation and microstructure characteristics were analyzed using X-ray diffraction and scanning electron microscopy, respectively. Our investigation aimed to establish a correlation between the dielectric behavior and optical properties to determine the optimal composition and conditions for utilizing BCZT as thermal detectors in electric vehicle battery packs. All BCZT powders exhibited a tetragonal phase, as confirmed by JCPDS No. 01-079-2265. We observed an increase in the dielectric constant with higher calcining temperatures or longer dwell times. Remarkably, BCZT0.85 ceramic sintered at 1250 °C for 4 h displayed the highest dielectric constant of 15,342, establishing this condition as optimal for preparing the dielectric film with a maximum dielectric constant of 42. Furthermore, we investigated the temperature-dependent electroluminescence intensity of the samples, revealing a significant enhancement with increasing temperature, reaching its peak at 80 °C. Additionally, we observed a positive correlation between electroluminescence intensity and dielectric constant, indicating the potential for improved opto-thermal sensors. The findings from this study offer promising opportunities for the development of advanced opto-thermal sensors with potential applications in electric vehicle battery packs. Our work contributes to the expanding field of photoluminescent and electroluminescent systems by providing novel insights into the design and optimization of efficient and reliable sensors for thermal monitoring in electric vehicle technologies.

12 February 2021 in Integrated Ferroelectrics
Verified
Journal Article
Closed access
OKOrawan Khamman
Orawan Khamman
PWPimpilai Wannasut
Pimpilai Wannasut
AWAnucha Watcharapasorn
Anucha Watcharapasorn
SASupon Ananta
Supon Ananta
The (1-x)Pb(Ni1/3Nb2/3)O3-xPb(Zr1/2Ti1/2)O3 (PNN-PZT) ceramic nanocomposites were fabricated via the bimodal particle sizes concept between nanosized PNN and micron-sized PZT powders. Crystal structure, microstructure and dielectric properties of all samples were investigated as a function of composition via a combination of X-ray diffraction (XRD), scanning electron microscopy (SEM) and dielectric spectroscopy techniques. It was found that, in general, the perovskite structure was formed. Broad dielectric transition maxima and high dielectric constant over a wide temperature range were obtained and could be attributed to the densification and compositional fluctuation derived from the employed bimodal particle size precursors.

12 June 2023 in Preprints.org
Verified
Preprint
Open access
PDF file
MKManlika Kamnoy
Manlika Kamnoy
KPKamonpan Pengpat
Kamonpan Pengpat
TTTawee Tunkasiri
Tawee Tunkasiri
OKOrawan Khamman
Orawan Khamman
UIUraiwan Intatha
Uraiwan Intatha
SESukum Eitssayeam
Sukum Eitssayeam
Photoluminescent (PL) layers and electroluminescent (EL) systems have been extensively explored for constructing flat panels, screen monitors, and lighting systems. Due to their optical properties, our group is interested in the relationship between optical properties and dielectric constant is converted due to thermal change. In this study, we prepared a zinc sulfide (ZnS) fluorescent film on barium-calcium zirconium titanate ceramics. BCZT0.85 (Ba0.85Ca0.15Zr0.1Ti0.9O3) and BCZT0.9 (Ba0.9Ca0.1Zr0.1Ti0.9O3) were prepared using the solid-state reaction method for the dielectric layer. The BCZT powders were calcined at 1200 and 1250 °C and dwell times of 2 and 4h. The phase formation and microstructure characteristics were then determined using X-ray diffraction and scanning electron microscopy, respectively. The dielectric behavior and optical properties rela-tionship was then studied to determine the composition and optimal conditions for further use as thermal detectors in electric vehicle battery packs. All BCZT powders exhibited the tetragonal phase, which was confirmed by JCPDS No. 01-079-2265. The dielectric constant increased with increasing calcining temperature or dwell time. The dielectric properties showed the BCZT0.85 ceramic sintered had the maximum dielectric constant of 15342 at calcine temperature of 1250 °C for 4h. Therefore, in this study, this condition was optimal for preparing the dielectric film. The maximum dielectric constant film is 42. The electroluminescence intensity of the samples increased in a temperature-dependent manner, with the highest EL intensity at 80 °C. Moreover, the electroluminescence intensity value was enhanced with the increase of the dielectric constant. Our results show promise for developing applications for Opto-thermal sensors.