Rheological property is very important for magnetorheological fluids, but tribological property also is a crucial factor to determine whether magnetorheological fluids can work stably. In order to find suitable carbonyl iron powder for magnetorheological fluids, three magnetorheological fluids are prepared by ordinary, reduced, and phosphated carbonyl iron powders, and their properties are compared. The microstructures of the different carbonyl iron powders are observed by scanning electron microscopy and X-ray diffraction. Sedimentation stability of the magnetorheological fluids is obtained by observation. The tribological and rheological properties are measured by friction testing machine and rotational rheometer. The results show that MRF-pho have superior tribological property and sedimentation stability, MRF-ord have higher shear yield stress, MRF-red have better comprehensive properties.
To investigate the effect of surface hardness on the wear characteristics of magnetorheological fluid, transmission components with different surface hardness levels are fabricated using four surface treatments: untreated, nickel-plated, low-temperature nitrided, and titanium-coated. This study focuses on the mechanism by which variations in surface hardness affect the wear behavior and the power transmission performance of magnetorheological fluid. The variation in the shear yield stress of magnetorheological fluid under different surface treatments is measured using a self-built experimental apparatus dedicated to magnetorheological fluid power transmission and wear testing. Furthermore, scanning electron microscopy was adopted to characterize the wear morphologies of both transmission surfaces and magnetic particles before and after the tests, while a white light interferometer was utilized to quantify variations in surface roughness. The experimental results demonstrate that the power transmission attenuation of magnetorheological fluid induced by nickel-plated, low-temperature nitrided, and titanium-coated surfaces is 14.01%, 4.67%, and 18.71%, respectively. Low-temperature nitrided and titanium-coated components can remarkably inhibit the wear of the transmission surface and effectively improve its wear resistance. However, titanium-coated transmission surfaces result in significant wear of the magnetic particles in the magnetorheological fluid. Therefore, low-temperature nitrided treatment of the surface can achieve both high shear yield stress and excellent wear resistance.
20 October 2026 in Journal of Intelligent Material Systems and Structures
To investigate the effect of magnetic field on the friction and wear characteristics of the transmission surface in magnetorheological fluid, the Archard wear model is modified by introducing the excitation current parameter. Then, surface wear during magnetorheological fluid transmission is simulated using Abaqus. The transmission performance at different excitation currents is tested using a self-developed magnetorheological fluid friction and wear experimental device. After the experiments, a scanning electron microscope and a white light interferometer are used to characterize the wear morphology of the transmission surface. The experimental results show that the wear depth on the outer region of the transmission surface is larger than that on the inner region. In addition, the wear on the transmission surface becomes more severe with higher excitation current. The conventional Archard model and the modified Archard model exhibit average relative errors of 20.61% and 9.56%, respectively. Therefore, the modified Archard wear model provides meaningful guidance for research on surface wear in magnetorheological fluid.