The changes in the set and concentration of optically active defects in brown natural diamonds subjected to high pressure and high temperature annealing are studied. The darker brown color of the studied samples corresponds to stronger plastic deformation. The activation energy of the dissociation of the nitrogen pairs (defects A) decreases from 6.0 ± 0.4 eV in colorless samples with weak plastic deformation to 3.7 eV in dark brown samples with strong deformation. Possible defect transformation mechanisms are discussed.
Tightly focused 515-nm, 0.3-ps laser pulses modify in a laser filamentation regime the crystalline structure of an Ib-type high-pressure, high-temperature (HPHT) synthesized diamond in a thin-plate form. The modified microregions (micromarks) in the yellow and colorless crystal zones, possessing different concentrations of elementary substitutional nitrogen (N) impurity atoms (C-centers), exhibit their strongly diminished local IR absorption (upon correction to the thickness scaling factor). Simultaneously, local visible-range (400–550 nm) absorption coefficients were increased, and photoluminescence (PL) yield was strongly enhanced in the broad range of 450–800 nm. The strong yellow-red PL enhancement saturates with laser exposure, implying the complete conversion of C-centers into nitrogen-vacancy (NV0,−) ones due to the laser-induced generation of Frenkel “interstitial-vacancy” I–V carbon pairs. The other emerging blue-green (>470 nm) and green-yellow (>500 nm) PL bands were also simultaneously saturated versus the laser exposure. The observed IR/optical absorption and PL spectral changes enlighten the ultrashort pulse laser inscription of NV0−-based quantum-emitter centers in synthetic diamonds and enable the evaluation of the productivity of their inscription along with the corresponding I–V generation rates.