In this experiment a cast iron alloy consisting of 0.019, 0.151, 0.431, and 0.646% niobium by weight was set and the microstructure solidification of iron with lamellar graphite was provided. These alloys were subjected to an abrasion test and chemical analyses of the microstructure were done by using scanning electron microscopy (SEM) and energy dispersive X-ray spectrometry (EDS). In addition to this, phase compositions were characterised by X-ray diffraction (XRD). Tests of mechanical strength, hardness, and tension were also applied to the alloys. The results of this experiment demonstrated that the addition of niobium to iron with lamellar graphite caused an increase in the abrasion resistance by 15%. This experiment shows that adding niobium improves the mechanical properties of grey cast iron.
In this study, grey cast iron (GG25) was produced via reinforcement with carbon titanium nitride (TiNC) in different amounts (0%, 0.153%, 0.204% and 0.255%). Samples were made from this material according to the standards for hardness, compression and wear, and then experiments were conducted. The test conditions applied for the TiNC-reinforced samples were similarly applied to unreinforced samples. The TiNC-reinforced and unreinforced samples were compared regarding their compression, hardness, and wear properties. The results of the hardness tests showed the highest average hardness value of 215 HB for sample A (0% TiNC). For TiNC-reinforced specimens, the hardness values of the reinforced specimens increased with increasing reinforcement. Sample B (0.153% TiNC) had an average hardness value of 193 HB. For sample C (0.204% TiNC), an average hardness value of 200 HB was measured. For sample D (0.255% TiNC), an average hardness value of 204 HB was determined. Sample A’s highest compression strength value was 780 MPA (0% TiNC). Similar to the hardness test values, the compression strength of the reinforced samples increased with the increasing reinforcement rate. The compression test value was found to be 747 MPa for sample B (0.153% TiNC), 765 MPa for sample C (0.204% TiNC) and 778 MPa for sample D (0.255% TiNC). Wear tests were performed on all samples to examine changes in the wear volume loss, wear rate and friction coefficients. Scanning electron microscopy (SEM) was used to determine the wear mechanisms on the worn surfaces of the samples. When examining the wear condition of the samples with the same hardness value as a function of increasing load values, increases in the wear volume loss values were observed as the load value increased.
9 June 2014 in Advances in Materials Science and Engineering
Gears made of plastic-based materials are anticorrosive, resistant to magnetic environments, and light and have pulse decay, low noise, and self-lubrication properties, and therefore their usage areas are widening every single day. In this experiment, the working conditions of 30% fibreglass PA 66 (PA 66 GFR 30) plastic material with PA 66 (PA 66 GFR 30) plastic material and AISI 8620 couple gear are observed. Usage of PA 66 GFR 30 material as gear material at 56.75 Nm constant load and 750 rpm, 1000 rpm, and 1500 rpm was analysed. The load capacity damage formation of the material was also analysed. The tooth surface temperature, corrosion depth of the tooth profile, tooth damage, and the tooth surface were examined with an scanning electron microscopy (SEM) and the corrosive behaviour of gears was analysed.
Steering gearbox bodies, which are produced from spheroidal graphite cast iron, experience wear and gaps over time since they operate under load. It is important to strengthen steering gearbox bodies to avoid this. In this study, a steering gearbox body was produced from a spheroidal graphite cast iron material with zirconium diboride at varying rates (0%, 0.227%, 0.455%, and 1.364%). Samples of the material were prepared according to established standards for hardness, compressive strength, and wear resistance tests. The mechanical properties of test samples with and without zirconium diboride (hardness, compressive strength, and wear resistance) were compared. Sample C showed the highest hardness measurement of 243 HB after adding 0.455% zirconium diboride. As the rate of addition increased, the values obtained from the hardness measurement test also increased. Sample C had the highest compressive value of 1438 MPa, with a 0.455% addition rate. It was found that the compressive strength values also increased as the addition rate increased. Wear tests were conducted to analyse wear volume, wear rate, and friction coefficients. A scanning electron microscope (SEM) device was utilised to identify wear mechanisms on the worn surfaces of the samples. Per the results of this study, wear volume values were found to increase with the load value.
AA7075 aluminum alloy was reinforced with B 4 C particles to produce aluminum composite materials. In the production of AA7075/B 4 C composite materials, semi-solid mixing methods were applied for homogen reinforcement dispersion then low pressure solidification. For the determination of the mechanical properties of the obtained samples; three point bending, compression and hardness tests were performed. In addition, microstructure, reinforcement matrix interface and chemical structure of the composite material produced by SEM, EDS, XRD analysis were examined. As a result, it was observed that; using the semi-solid mixing method the reinforcing powders could be distributed homogeneously into the matrix, both chemical and mechanical bonding could be occurs between the matrix and the reinforcing material and this mixing technique could be easily used in the production of particle reinforced metal composites.