Given the rising upscaling trend in lithium-ion battery (LiB) production, there is a growing emphasis on the environmental and economic impacts alongside the high energy density demands. The cost and environmental impact of battery production primarily arise from the critical elements Ni, Co, and F. This drives the exploration of Ni-free and Co-free cathode alternatives such as LiMn2O4 (LMO) and LiFePO4 (LFP). However, the absence of Ni and Co results in reduced capacity and insufficient cyclic stability, particularly in the case of LMO due to Mn dissolution. To compensate for both low cathode capacitance and low cycle stability, we propose the GREENcell, a lithium cell combining a F-free polyisobutene (PIB) binder-based LMO cathode with a stabilized in -situ LiAL alloy anode. A LiAl alloy anode with the chemical composition of LiAl already shows a theoretical capacity of 993 Ah·kg−1. Therefore, it promises extraordinarily higher energy densities compared to a commercial graphite anode with a capacity of 372 Ah·kg−1. Following an iterative development process, different optimization strategies, especially those targeting the stability of the Al-based anode, were evaluated. During Al foil selection, foil purity and thickness could be identified as two of the dominant influencing parameters. A pressed-in stainless steel mesh provides both mechanical stability to the anode and facilitates alloy formation by breaking up the Al oxide layer beforehand. Additionally, a binder-stabilized Al oxide or silicate layer is pre-coated on the Al surface, posing as a SEI-precursor and ensuring a uniform liquid electrolyte distribution at the phase boundary. Employing a commercially available Si-containing Al alloy mitigated the mechanical degradation of the anode, yielding a favorable impact on long-term stability. The applicability of the novel optimized GREENcell is demonstrated using laboratory coin cells with LMO and LFP as the cathode. As a result, the functionality of the GREENcell was demonstrated for the first time, and thanks to the anode stabilization strategies, a capacity retention of >70% after 200 was achieved, representing an increase of 32.6% compared to the initial Al foil.
The novelty of this work lies in the optimization of the GREENcell-concept by combining a strain-hardened and passivated Al alloy foil anode with a F-free LiMn 2 O 4 cathode for achieving a commercially viable, low-cost, and sustainable LiB.
14 October 2026 in Journal of the Electrochemical Society
Aluminum (Al) foil anodes are promising candidates for sustainable lithium‐ion batteries (LiB) thanks to their high theoretical capacity (993 mAh·g −1 ) and inherently coating‐free, foil-based architecture. Their practical implementation, however, is hindered by pronounced mechanical degradation and insufficient cycling stability. Within the GREENcell -concept, we investigated two fully scalable stabilization strategies that rely exclusively on commercially available Al alloy foils, paired with a fluorine (F)‐free polyisobutylene (PIB) binder-based LiMn 2 O 4 (LMO) cathode: (1) plating a nickel (Ni) layer onto the Al alloy foil 8011 surface as an additional current collector and (2) using commercially available high silicon (Si)-content Al alloy foil 4343 with 7.5 wt% Si-content. Full-cell and half-cell measurements combined with electrochemical impedance spectroscopy, and post-mortem morphological analysis correlate the electrochemical performance to structural evolution. Owing to improvement in the homogenous current distribution and enhanced mechanical stability, the plated Ni on the Al alloy foil 8011 reduces the initial capacity loss, lowers the ohmic resistance, and suppresses crack propagation during prolonged cycling, resulting in a 15 % increase in capacity retention after 100 cycles relative to the untreated Al alloy foil. In contrast, the Ni-plated high Si-content Al alloy foil 4343 exhibits higher initial irreversible losses but undergoes a more pronounced activation in the intermediate cycling stage, accompanied by enhanced diffusion-controlled kinetics. As a result, it achieves a capacity retention of 67 % after 100 cycles, corresponding to a total improvement of 24 % compared with the untreated low Si-content Al reference 8011. These findings establish practical design principles for Al-based anodes and further advance the GREENcell -concept toward cost-efficient, scalable, and industrially viable next-generation LiBs.