Taguchi’s method was applied to investigate the effect of main high energy ball milling (HEBM) parameters: milling time (MT), ball to powder weight ratio (BPWR), and milling speed (MS) on the CaCO3 crystallite size. The settings of HEBM parameters were determined by using the L9 (33) orthogonal experiments array (OA). The as-received and milled powders were characterized by X-ray diffraction (XRD) scanning electron microscopy (SEM), Fourier transform infrared (FTIR) spectroscopy. The crystallite size of CaCO3 varied between 140 and 540 nm depending on the HEBM conditions. The analysis of variance (ANOVA) was used to find the significance and percentage of contribution of each milling parameter. It was established that the MT is the most effective parameter followed by MS and BPWR. A confirmation test was carried out with a 90% confidence level to illustrate the effectiveness of the Taguchi optimization method. The optimum milling parameter combination was determined by using the analysis of signal-to-noise (S/N) ratio. Based on the S/N ratio analysis, optimal HEBM conditions were found MT 10 h, MS 600 revolutions per minute (rpm), BPWR 50:1.
Nano-silica (NS) is used to enhance the mechanical and durability properties of cementitious materials; however, its frequent tendency to agglomerate limits its effectiveness and uniform distribution within the cement matrix. The main goal of this study was to improve NS dispersion and therefore to improve the properties of the concrete by coating NS onto standard sand particles (sand@NS) using the Stöber method, creating a composite material that acts as a filler, nucleation site, and highly reactive pozzolanic agent. The resulting sand@NS was incorporated into cement mixtures, and its compressive strength was measured after 3, 7, and 28 days of curing. In addition, water absorption and microstructural density were also evaluated. Comparative results showed that sand@NS significantly enhanced early-age hydration and initial strength, with a 145% increase in compressive strength at 28 days compared to the reference, whereas free NS resulted in a 120% increase. The early-age strength improvement was mainly due to the increased number of nucleation centers, while later strength gains were attributed to pozzolanic activity of the immobilized NS. Additionally, sand@NS reduced water absorption and increased microstructural density, even with reduced cement content, supporting more sustainable and eco-efficient concrete production. This work shows a promising, scalable, and cost-effective strategy to maximize the performance of NS in cementitious systems and supports its broader adoption in advanced construction materials.