Intrinsically stretchable light-emitting materials are crucial for skin-like wearable displays; however, their color range has been limited to green-like yellow lights owing to the restricted stretchable light-emitting materials (super yellow series materials). To develop skin-like full-color displays, three intrinsically stretchable primary light-emitting materials [red, green, and blue (RGB)] are essential. In this study, we report three highly stretchable primary light-emitting films made from a polymer blend of conventional RGB light-emitting polymers and a nonpolar elastomer. The blend films consist of multidimensional nanodomains of light-emitting polymers that are interconnected in an elastomer matrix for efficient light-emitting under strain. The RGB blend films exhibited over 1000 cd/m 2 luminance with low turn-on voltage (<5 Von ) and the selectively stretched blend films on rigid substrate maintained stable light-emitting performance up to 100% strain even after 1000 multiple stretching cycles.
Conjugated polymers have been widely investigated where ladder-type conjugated polymers receive more attention due to their rigid backbones and extraordinary properties. However, the understanding of how the rigid conformation of ladder polymers translates to material properties is still limited. Here, we systematically investigated the solution aggregation properties of a carbazole-derived conjugated ladder polymer (LP) and its analogous non-ladder control polymer (CP) via light scattering, neutron scattering, and UV-vis absorption spectroscopy characterization techniques, revealing a highly robust, temperature-insensitive aggregation behavior of the LP. The experimental findings were further validated by computational molecular dynamics simulations. We found that the peak positions and intensities of the UV spectra of the LP remained constant between 20 °C and 120 °C in chlorobenzene solution. The polymer also showed a stable hydrodynamic radius measured by dynamic light scattering from 20 °C to 70 °C in the chlorobenzene solution. Using small-angle neutron scattering, no Guinier region was reached in the measured q range down to 0.008 Å−1, even at elevated temperature. In contrast, the non-ladder control polymer CP was fully soluble in the chlorobenzene solvent without the observation of any notable aggregates. The Brownian dynamics simulation showed that during polymer aggregation, the entropy change of the LP was significantly less negative than that of the non-ladder control polymer. These findings revealed the low entropy nature of rigid conjugated ladder polymers and the low entropy penalty for their aggregation, which is promising for highly robust intermolecular interactions at high temperatures. Such a unique thermodynamic feature of rigid ladder polymers can be leveraged in the design and application of next-generation electronic and optoelectronic devices that function under unconventional high temperature conditions.
Conjugated polymers (CPs) are solution-processible for various electronic applications, where solution aggregation and dynamics could impact the morphology in the solid state. Various solvents and solvent mixtures have been used to dissolve and process CPs, but few studies have quantified the effect of solvent quality on the solution behavior of CPs. Herein, we performed static light scattering and small-angle X-ray scattering combined with molecular dynamics (MD) simulation to investigate CP solution behaviors with solvents of varying quality, including poly(3-alkylthiophene) (P3ATs) with various sidechain lengths from –C4H9 to –C12H25, poly[bis(3-dodecyl-2-thienyl)-2,2′-dithiophene-5,5′-diyl] (PQT-12) and poly[2,5-bis(3-dodecylthiophen-2-yl)thieno[3,2-b]thiophene] (PBTTT-12). We found that chlorobenzene is a better solvent than toluene for various CPs, which was evident from the positive second virial coefficient A2 ranging from 0.3 to 4.7 × 10−3 cm3 mol g−2 towards P3ATs. For P3ATs in non-polar solvents, longer sidechains promote more positive A2, indicating a better polymer–solvent interaction, wherein A2 for toluene increases from −5.9 to 1.4 × 10−3 cm3 mol g−2, and in CB, A2 ranges from 1.0 to 4.7 × 10−3 cm3 mol g−2 when sidechain length increases from –C6H13 to –C12H25. Moreover, PQT-12 and PBTTT-12 have strong aggregation tendencies in all solutions, with an apparent positive A2 (∼0.5 × 10−3 cm3 mol g−2) due to multi-chain aggregates and peculiar chain folding. These solvent-dependent aggregation behaviors can be well correlated to spectroscopy measurement results. Our coarse-grained MD simulation results further suggested that CPs with long, dense, and branched sidechains can achieve enhanced polymer–solvent interaction, and thus enable overall better solution dispersion. This work provides quantitative insights into the solution behavior of conjugated polymers that can guide both the design and process of CPs toward next-generation organic electronics.
Thermal conductivity directly impacts the performance of organic thermoelectric devices which convert heat into useful electricity. However, quantitatively measuring the bulk thermal conductivity of conjugated polymers remains complicated and hinders the rational design of advanced organic thermoelectric materials and true key performance calculation, figure of merit (ZT). The novel fast scanning calorimetry is adopted to address these limitations for the first time by measuring the heat conduction for conjugated polymeric films. Out of plane thermal conductivity of polydiketopyrrolopyrrole (PDPPT) based polymers and poly (3-hexylthiophene) (P3HT) films are quantitatively captured by directly monitoring heat transfer through tens of micrometer thick polymer films. For undoped polymers, PDPPT displayed a higher out of plane thermal conductivity than P3HT (0.263 vs. 0.168 W m−1 K−1) due to higher backbone rigidity. After doping with 2,3,5,6-tetrafluoro-7,7,8,8-tetracyanoquinodimethane (F4TCNQ), the thermal conductivity of doped PDPPT first increases at lower doping levels up to 5 wt%, and then decreases at higher doping levels, which can be attributed to changes in the degree of crystallinity for doped films quantified by X-ray scattering measurements. The highest thermal conductivities are found for doping levels ranging from of 2.5% for P3HT (0.276 W m−1 K−1) and 5% for PDPPT (0.420 W m−1 K−1) primarily due to the enhanced degree of crystallinity. This work further facilitates the rational design of future organic thermoelectric materials by optimizing the thermal conductivity using controlled doping.
Hierarchically macro-/mesoporous (HMM) materials generally contain at least two distinct populations of pore sizes with ranges of 2–50 nm and >50 nm; they exhibit promising performance for various applications, such as water remediation and energy storage, due to the combined advantages of high surface area, pore accessibility, and porosity. Conventional synthesis of HMM materials typically utilize multiple templating agents to develop varied sizes of pores, often involving complex processes and the use of relatively expensive precursors with low recourse-efficiency, leading to significant challenges toward scaled production. Therefore, development of a simple approach for HMM materials synthesis is important for facilitating their commercialization and broad use. In this work, we demonstrate a generalizable method for the fabrication of HMM polymers and carbons using immiscible thermoplastic elastomer (TPE) blends, through incorporating a small amount of polystyrene-block-polyisoprene-block-polystyrene (SIS) within the matrix of polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene (SEBS), followed by sulfonation-induced crosslinking. During this reaction, the presence of SIS not only leads to the formation of macropores from released gaseous products, but it also facilitates the selective degradation of polystyrene domains to develop ordered mesopores. These porous polymers can then be converted to HMM carbons upon pyrolysis, where ordered nanostructures can be retained. This approach to produce HMM materials can be generalized to different selections of TPE blends with varied precursor identity and molecular weight. Furthermore, we demonstrate that HMM polymers can be employed as sorbents for the efficient removal of heavy metals from aqueous systems, while their derived carbons are efficient for organic pollutant remediation. We believe this work demonstrates a simple and robust approach with great potential for the scaled manufacturing of HMM materials to enable their broad use in practical applications.