Synthetic materials reinforced with natural fibers are attracting great attention of scientists and researchers. Sustainability and eco‐friendly nature along with easy availability and low cost are the key reasons. In this work, a natural fiber such as a banana fiber was investigated to create bioavailable materials while enhancing mechanical properties. The banana fiber was extracted from banana sheath by the mechanical method combined with chemical treatment with NaOH 1, 2, 3, 4, and 5%. Treatment of the banana fiber with NaOH effectively removes other impurities from the fiber surface and the fiber surface becomes rough, increasing the compatibility and bonding between banana fiber and PLA. The reported optimum NaOH concentration was 5% banana fiber used for the material polylactic acid (PLA) composite/banana fiber. The composites (BF) were prepared by the hot melt mixing method. The results showed that 20% by weight of banana fiber gave good results and the mechanical strength values kept at the specified level (tensile strength: 52.57 MPa, flexural strength: 70.35 MPa, impact strength: 155.45 J/m and hardness: 23.8 Hv). SEM observations showed visual evidence that surface impurities were removed from the fiber by NaOH treatment.
22 July 2021 in International Journal of Chemical Engineering
Currently, the growing field of technology has paved the way for using environmental friendly resources; in particular, plant origin holds ecological concern and renewable aspects. Currently, natural fiber composites have widening attention, thanks to their eco-friendly properties. In the present work, the composite material is reinforced with natural fibers from the bark of banana trees (banana fibers), a material available in Vietnam. Banana fibers are extracted from banana peels, pretreated with NaOH 5%, and then cut to an average length of 30 mm. Banana fiber is reinforced for epoxy resin Epikote 240 with mass percents: 10 wt.%, 15 wt.%, 20 wt.%, and 25 wt.%. The results were evaluated through structural morphology (SEM), mechanical properties, fire resistance, and thermal properties. Experimental results show that the tensile, compressive, and impact strengths of biosynthetic materials up to 20% by weight have increased compared to epoxy neat. Flame retardant and thermal properties are kept stable; 20 wt.% banana fiber gives a limiting oxygen index of 20.8% and satisfactory thermal stability.
Docynia indica (D. indica) shows various useful biological activities, such as antioxidant, anti-inflammatory, antibacterial effects, and positive benefits for human health. Such biological activities relate to the main phytochemicals of D. indica including phenolic and flavonoid. However, isolation for phenolic and flavonoid by popular methods such as hot extraction, soxhlet extraction, and ultrasonic extraction have been relatively ineffective. Therefore, in this study, microwave-assisted extraction (MAE) was used for the extraction of total phenolic and total flavonoid from D. indica. The optimization experiments were conducted based on response surface methodology (RMS) according to a central composite design with four independent variables: extraction time (min), ethanol concentration (%, v/v), microwave power (W), and pH of the solvent. Three dependent variables were total phenolic content (TPC), total flavonoid content (TFC), and yield. The optimal conditions for the extraction of phenolic and flavonoid from D. indica were: extraction time of 50 min, ethanol concentration of 65%, microwave power of 440 W, and solvent pH of 5.4. These conditions corresponded to TPC, TFC, and yield values of 33.57 ± 0.12 (mg GAE/g), 25.01 ± 0.11 (mg QE/g) and 33.44 ± 0.14 (%), respectively.
25 June 2021 in International Journal of Chemical Engineering
Studies on using biomaterials hybridized with other materials to produce biomaterials have been paid more attention due to their low cost, abundance, renewability, and degradability. Therefore, these materials are ecofriendly and nontoxic to humans. A large number of used coffee grounds (SCGs) are often discarded and replacements are necessary for dealing with environmental problems. This work developed sustainable materials by reusing SCGs. Used coffee grounds were mixed with epoxy resin at different amounts: 30 wt , 40 wt , 50 wt , and 60 wt . SCGs were treated with 0.5N NaOH, at SCGs/NaOH ratio of 1:2. SEM images showed that the material with 30 wt SCGs has good compatibility without phase division on the SCGs-epoxy interface. Results of mechanical properties of epoxy composites with 30 wt SCGs are as follows: tensile strength of 44.81±10MPa, flexural strength of 80.07±0.16MPa, compressive strength of 112.56±0.11MPa, and Izod strength and impact of 8.21±0.19kJ/m2. In terms of flame-retardant properties, the oxygen index is limited to 20.8±0.20 and the burning rate according to UL94HB is 27.02±0.29mm/min. The obtained results indicate that it is possible to produce biohybrid composites from epoxy resin and SCGs. This work offers an ecofriendly alternative method to use the waste of the coffee industry. It contributes to improvements of the general characteristics of composites such as mechanical, thermal, and flame-retardant properties. This work proved that SCGs have a high potential to be used in a wide range of composite materials for civil engineering applications.
This paper reports the improvement of the mechanical properties and flame retardant properties of epoxy Epikote 240/nanoclay I.30E/multiwalled carbon nanotube nanocomposite prepared by mechanical stirring method combined with ultrasonic vibration, nanoclay I.30E content (1; 2; 3 wt.%) and content of MWNT (0.01; 0.02; 0.03 wt.%). When burned, MWCNT reduces degradation speed of epoxy Epikote 240 resin and increases the char yield, and nanoclay acts as an energy storage medium to hinder the heat transfer in epoxy resin. The limiting oxygen index value and UL94 test indicated improvement of flame retardancy of the nanocomposites. The results exhibit the potentiality of these based epoxy Epikote 240 resin/nanoclay I.30E/MWCNTs nanocomposites for multifaceted advanced applications. These fillers can produce environmental friendly products with high thermal and mechanical properties.
Small and light fly ash is a by-product of thermal power plants, in which oxides mainly present in fly ash are suitable to reinforce composite materials. Its content accounts for 10, 20, 30, 40, and 50 of those materials. However, due to the smooth surface, it cannot stick completely in plastics. Therefore, in this work, it was studied to combine nanoclay additive (I.30E) with 1, 3, and 5 by weight to synergize to improve mechanical strength, fire retardation, and electrical properties. Mechanical properties and flame retardant properties have improved markedly. At the combined ratio of 40 by weight of fly ash and 3 nanoclay, nanocomposites have tensile strength values of 64.12MPa, flexural strength of 89.27MPa, compressive strength of 215.23MPa, and impact resistance of Izod 14.45kJ/m2, oxygen index limited to 26.8 of fire retardant material. In terms of dielectric strength, the electric strength of pure epoxy is 17.5kV/mm, higher than that before adding nanoclay (12.7kV/mm). The presence of nanoclays in the material creates a tortuous electric path, slowing the propagation of the power plant, which is the main factor that improves the breaking strength of the nanocomposite.