1 June 2019 in APL Materials
Verified
Journal Article
Open access
PDF file
APA. Y. Polyakov
A. Y. Polyakov
Inhwan LeeInhwan Lee
Inhwan Lee
NSN. B. Smirnov
N. B. Smirnov
EYEugene Yakimov
Eugene Yakimov
ISI. V. Shchemerov
I. V. Shchemerov
SPStephen Pearton
Stephen Pearton
Films of β-Ga2O3 grown by halide vapor phase epitaxy on native substrates were subjected to Ar inductively coupled plasma treatment. As a result, the built-in voltage of Ni Schottky diodes deposited on the plasma treated surfaces decreased from 1 V to −0.02 V due to the buildup of deep trap concentration in the near surface region. Deep level spectra measurements indicate a strong increase in the top ∼200 nm of the plasma treated layer of the concentration of E2* (Ec − 0.8 eV) and especially E3 (Ec − 1.05 eV) deep electron traps. Capacitance-voltage profiling with monochromatic illumination also indicated a large increase in the upper ∼100 nm of the film in the concentration of deep acceptors with optical threshold for an ionization of ∼2.3 eV and 3.1 eV. Such defects at the surface led to a significant increase in reverse current, an increase in the ideality factor in forward current, and a dramatic decrease in the diffusion length of nonequilibrium charge carriers from 450 nm to 150 nm.

15 July 2019 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
APA. Y. Polyakov
A. Y. Polyakov
Inhwan LeeInhwan Lee
Inhwan Lee
NSN. B. Smirnov
N. B. Smirnov
EYEugene Yakimov
Eugene Yakimov
ISI. V. Shchemerov
I. V. Shchemerov
SPStephen Pearton
Stephen Pearton
The effects of hydrogen plasma treatment of β-Ga2O3 grown by halide vapor phase epitaxy and doped with Si are reported. Samples subjected to H plasma exposure at 330 °C developed a wide (∼2.5 μm-thick) region near the surface, depleted of electrons at room temperature. The thickness of the layer is in reasonable agreement with the estimated hydrogen penetration depth in β-Ga2O3 based on previous deuterium profiling experiments. Admittance spectroscopy and photoinduced current transient spectroscopy measurements place the Fermi level pinning position in the H treated film near Ec-1.05 eV. Annealing at 450 °C decreased the thickness of the depletion layer to 1.3 μm at room temperature and moved the Fermi level pinning position to Ec-0.8 eV. Further annealing at 550 °C almost restored the starting shallow donor concentration and the spectra of deep traps dominated by Ec-0.8 eV and Ec-1.05 eV observed before hydrogen treatment. It is suggested that hydrogen plasma exposure produces surface damage in the near-surface region and passivates or compensates shallow donors.

5 January 2020 in ECS Journal of Solid State Science and Technology
Verified
Journal Article
Open access
APAlexander Y. Polyakov
Alexander Y. Polyakov
VNV. I. Nikolaev
V. I. Nikolaev
SSS. I. Stepanov
S. I. Stepanov
APA. I. Pechnikov
A. I. Pechnikov
EYE. B. Yakimov
E. B. Yakimov
SPStephen Pearton
Stephen Pearton
Films of α-Ga2O3 doped with Sn were grown by halide vapor phase epitaxy (HVPE) on planar and patterned sapphire substrates. For planar substrates, with the same high Sn flow, the total concentration of donors was varying from 1017 cm−3 to high 1018 cm−3. The donor centers were shallow states with activation energies 35–60 meV, centers with levels near Ec–(0.1–0.14) eV (E1), and centers with levels near Ec–(0.35–0.4) eV (E2). Deeper electron traps with levels near Ec−0.6 eV (A), near Ec−0.8 eV (B), Ec−1 eV (C) were detected in capacitance or current transient spectroscopy measurements. Annealing of heavily compensated films in molecular hydrogen flow at 500 °C for 0.5 h strongly increased the concentration of the E1 states and increased the density of the E2 and A traps. For films grown on patterned substrates the growth started by the formation of the orthorhombic α-phase in the valleys of the sapphire pattern that was overgrown by the regions of laterally propagating α-phase. No improvement of the crystalline quality of the layers when using patterned substrates was detected. The electric properties, the deep traps spectra, and the effects of hydrogen treatment were similar to the case of planar samples.

1 May 2019 in APL Materials
Verified
Journal Article
Open access
PDF file
APA. Y. Polyakov
A. Y. Polyakov
NSN. B. Smirnov
N. B. Smirnov
ISI. V. Shchemerov
I. V. Shchemerov
EYEugene Yakimov
Eugene Yakimov
VNV. I. Nikolaev
V. I. Nikolaev
SPStephen Pearton
Stephen Pearton
Epitaxial layers of α-Ga2O3 with different Sn doping levels were grown by halide vapor phase epitaxy on sapphire. The films had shallow donor concentrations ranging from 1017 to 4.8 × 1019 cm−3. Deep level transient spectroscopy of the lowest doped samples revealed dominant A traps with level Ec − 0.6 eV and B traps near Ec − 1.1 eV. With increasing shallow donor concentration, the density of the A traps increased, and new traps C (Ec − 0.85 eV) and D (Ec − 0.23 eV) emerged. Photocapacitance spectra showed the presence of deep traps with optical ionization energy of ∼2 and 2.7 eV and prominent persistent photocapacitance at low temperature, surviving heating to temperatures above room temperature. The diffusion length of nonequilibrium charge carriers was 0.15 µm, and microcathodoluminescence spectra showed peaks in the range 339–540 nm, but no band-edge emission.

5 May 2020 in Journal of Physics D: Applied Physics
Verified
Journal Article
Closed access
APA Y Polyakov
A Y Polyakov
NSN B Smirnov
N B Smirnov
ISI V Shchemerov
I V Shchemerov
AVAnton Vasilev
Anton Vasilev
EYE B Yakimov
E B Yakimov
SPStephen Pearton
Stephen Pearton
The effects of pulsed neutron irradiation on Si doped n-type β-Ga 2 O 3 films grown by halide vapor phase epitaxy (HVPE) on bulk Sn doped n + β-Ga 2 O 3 substrates are reported. This irradiation leads to an almost linear increase with neutron fluence of the density of deep electron traps E2* (E c − 0.74 eV), E3 (E c − 1.05 eV), and E4 (E c − 1.2 eV), with an introduction rate close to 0.4–0.6 cm −1 while the density of the E2 traps (E c − 0.8 eV) related to Fe was virtually unchanged. In addition, the increase in the density of deep traps with optical ionization threshold of 1.3 eV, 2.3 eV, and 3.1 eV with an introduction rate close to 0.8–2 cm −1 was observed. The carrier removal rate under our conditions was 28 cm −1 . Neutron irradiation also led to a measurable decrease of the diffusion length of nonequilibrium charge carriers. The results are qualitatively similar to previous reports for proton and α-particle irradiation of HVPE β-Ga 2 O 3 . When comparing the findings with those described earlier for bulk neutron irradiated Ga 2 O 3 , we observe lower starting densities of electron and hole traps and lower introduction rates for these traps in the epitaxial structures. The carrier removal rates were comparable to those in bulk crystals.

1 June 2022 in APL Materials
Verified
Journal Article
Open access
PDF file
APAlexander Y. Polyakov
Alexander Y. Polyakov
VNV. I. Nikolaev
V. I. Nikolaev
APA. I. Pechnikov
A. I. Pechnikov
Sergey I. StepanovSergey I. Stepanov
Sergey I. Stepanov
EYEugene Yakimov
Eugene Yakimov
SPStephen Pearton
Stephen Pearton
Thick (23 µm) films of κ-Ga2O3 were grown by Halide Vapor Phase Epitaxy (HVPE) on GaN/sapphire templates at 630 °C. X-ray analysis confirmed the formation of single-phase κ-Ga2O3 with half-widths of the high-resolution x-ray diffraction (004), (006), and (008) symmetric reflections of 4.5 arc min and asymmetric (027) reflection of 14 arc min. Orthorhombic κ-Ga2O3 polymorph formation was confirmed from analysis of the Kikuchi diffraction pattern in electron backscattering diffraction. Secondary electron imaging indicated a reasonably flat surface morphology with a few (area density ∼103 cm−2) approximately circular (diameter ∼50–100 µm) uncoalesced regions, containing κ-Ga2O3 columns with in-plane dimensions and a height of about 10 µm. Micro-cathodoluminescence (MCL) spectra showed a wide 2–3.5 eV band that could be deconvoluted into narrower bands peaked at 2.59, 2.66, 2.86, and 3.12 eV. Ni Schottky diodes prepared on the films showed good rectification but a high series resistance. The films had a thin near-surface region dominated by Ec − 0.7 eV deep centers and a deeper region (∼2 µm from the surface) dominated by shallow donors with concentrations of ≤1016 cm−3. Photocurrent and photocapacitance spectra showed the presence of deep compensating acceptors with optical ionization energies of ∼1.35 and 2.3 eV, the latter being close to the energy of one of the MCL bands. Deep level transient spectroscopy revealed deep traps with energies near 0.3, 0.6, 0.7, 0.8, and 1 eV from the conduction band edge. The results show the potential of HVPE to grow very thick κ-Ga2O3 on GaN/sapphire templates.