This study aimed to compare the effect of artificial saliva (AS) aging on the trueness and precision of direct-printed aligners vs thermoformed aligners. Four types of aligners were manufactured from the same reference standard tessellation language (STL) file: using Duran Plus (n = 12) for thermoformed ones, and TC-85DAC (n = 12), Clear A (n = 12), or OD Clear TF (OC, n = 12) resins for direct-printed ones. A printed model was used for thermoformed aligners, whereas digital design models were generated for direct-printed aligners from the reference STL file. The samples were sprayed and scanned (Trios 3; 3 Shape, Copenhagen, Denmark) before and after aging in AS at 37°C for 24 hours, 7 days, and 14 days. STL files were imported into CloudCompare software (CloudCompare, 2.13.2 version, Paris, France) and superimposed on the design or digital model (trueness) or to each other within each group (precision) using a 7 reference-point algorithm. Two-way analysis of variance was performed to evaluate the influence of saliva aging and material type. A significant effect of the material type was observed with a lower trueness and precision for Duran Plus aligners compared with the 3 groups of direct-printed aligners. A significant effect of AS aging, with a decrease of trueness and precision, was also noted for both thermoformed and printed aligners. This in vitro study demonstrated that direct-printed aligners provided higher trueness and precision than thermoformed ones. Exposure to AS decreased the trueness and precision for both types. However, further studies are needed to validate the behaviors of direct-printed aligners clinically.
This chapter reviews several cases of methacrylate-based polymers used for medical applications. The main chemicals and fillers used for elaborating biomaterials are presented, together with the main synthesis reactions. Their properties are recalled and discussed using the well-established structure–properties relationships of polymer physicochemistry. Last, the main degradation mechanisms are recalled, together with their consequences on the engineering properties of polymethacrylates, in order to predict the long-term in vivo behavior of such complex materials.
18 August 2025 in European Journal of Oral Sciences
This study investigated the influence of 10‐methacryloyloxydecyl dihydrogen phosphate (MDP) agents and repeated saliva contamination on the microtensile bond strength (µTBS) of two self‐adhesive resin cements (SARCs) bonded to dentin. Forty‐eight sound human teeth were randomly divided into eight experimental groups, based on three factors: the type of SARC, the presence or absence of an MDP agent, and the presence or absence of multiple saliva exposures. The control group for each SARC received neither MDP agent nor multiple saliva contaminations. For each group, five teeth were sectioned to obtain 30–44 beams, followed by µTBS testing, fracture mode analysis, and scanning electron microscopy. Data were analyzed using one‐way and two‐way analysis of variance, Scheffé’s test, and Weibull statistics. Under uncontaminated conditions, the application of MDP agents was found to significantly enhance the bond strength of both SARCs. Saliva contamination significantly reduced µTBS, regardless of the cement used. However, when MDP agents were applied prior to bonding, µTBS values remained comparable to those of uncontaminated controls, even after multiple saliva exposures. These results support the use of MDP agents to maintain adhesive integrity in the presence of repeated salivary contaminations, offering greater reliability in adverse clinical environments.
This study evaluated whether adjunctive 10‐methacryloyloxydecyl dihydrogen phosphate (MDP) primers enhance the microtensile bond strength (µTBS) of two universal adhesives (UAs) to dentin under artificial aging and repeated salivary contamination applied at each bonding step. One hundred fifty‐two human molars were assigned to 24 groups based on UA type, MDP primer application, contamination, and aging period (1, 30, and 180 d). Resin–dentin beams were sectioned and loaded to failure to determine µTBS. Failure modes were analyzed, and scanning electron microscopy (SEM) was used to assess hybrid layer quality and interfacial morphology. FTIR–ATR evaluated the effect of MDP primers on the degree of conversion (DC). Data were analyzed using one and three‐way anova , Scheffé’s test, and Weibull statistics. Under uncontaminated conditions, MDP primers significantly increased µTBS for both UAs after 180 d. Repeated contamination significantly reduced µTBS; however, adjunctive MDP priming restored bond strength to levels comparable to uncontaminated controls. FTIR–ATR demonstrated higher DC in MDP primer groups, suggesting enhanced interfacial polymerization. Weibull analysis confirmed improved bonding reliability with primer use. SEM revealed continuous hybrid layers in MDP groups regardless of contamination, whereas failure modes shifted toward more cohesive patterns. Adjunctive MDP priming mitigates the adverse effects of salivary contamination and aging on UA‐dentin bonding.