The sensitization behavior of the welding heat affected zone (HAZ) in austenitic stainless steels (SSs) was investigated through simulated thermal cycles emulating actual multi-pass welding processes using the Gleeble simulator. The tests were performed with austenitic SSs, considering carbon contents, heat input, and distance from the fusion line to determine the thermal cycle conditions of the HAZ. Higher carbon content led to increased sensitization (degree of sensitization, DOS) values, while the influence of the thermal cycle in the final weld pass was that even though it was rapidly heated to over 1000 °C and cooled at a rapid rate, the DOS value decreased due to partial carbide dissolution and chromium diffusion. Therefore, effective management of the final thermal cycle in the HAZ contributes to improved intergranular stress corrosion cracking resistance. Even with prolonged exposure of the HAZ to the sensitization region, the discovery that corrosion resistance improves when the final heating cycle reaches 1000 °C underscores the importance of HAZ heat cycle management and provides valuable insights for materials engineering and industrial applications. Graphical abstract
This study investigated the effect of the initial grain size on the laser beam weldability of CoCrFeMnNi high-entropy alloys (HEAs). Cold-rolled, annealed, and cast HEAs with different initial grain sizes exhibited clear differences in weldability. The cold-rolled, annealed, and cast HEAs exhibited grain sizes of 1.5, 8.1, and 1.1 mm, respectively. The grain size of the weld metal (WM) in cold-rolled/annealed HEAs was coarser than that of the base metal (BM), whereas the grain size of the WM in the cast HEA was finer than that of the BM. Shrinkage voids were present in the central region of all laser WMs. The cold-rolled and annealed HEA exhibited a tensile strength greater than 600 MPa owing to the grain size of the coarse WM and the presence of shrinkage voids; however, tensile fracture occurred in the central region of the WM. However, because the grain size of the cast HEA BM was finer than that of the WM, the tensile fracture occurred in the BM, and it had the same tensile properties as the BM. Therefore, the laser weldability of the HEA depended on the initial grain size, and the grain refinement of the WM was essential for improving the weldability.
This study investigated the microstructural and compositional behavior of Fe-Cr-Si clads produced in stainless steel (STS) 316 L with a decreased laser traverse speed using directed energy deposition (DED). The substrate of all specimens was mostly composed of austenite, while the clad region consisted of the δ-ferrite, martensite, and a small amount of retained austenite. The reduced heat input by increasing the laser traverse speed resulted in decreased dilution of the Ni component and the substrate’s unmixed zone, resulting in a gradual decrease (16−1%) in the face-centered cubic (FCC: austenite) phase of the clad region. In addition, in the clad region composed of body-centered cubic (BCC), the fraction of martensite decreased, but the fraction of the δ-ferrite increased by decreasing the heat input. The reason for this was that dense martensite was formed in the entire clad region owing to a sufficient cooling rate for phase transformation and dilution of the Ni component in the 12 mm/s specimen with the highest heat input. Therefore, to predict the corrosion and wear characteristics of the Fe-Cr-Si multilayer clad manufactured in STS316L, the formation of martensite by the dilution of the Ni component should be sufficiently considered.