Nanoporous silicon oxide templates formed by swift heavy ion tracks technology have been investigated. The influence of the heavy ion characteristics, such as type of ion, energy, stopping power and irradiation fluence on the pore properties of the silicon oxide templates, has been studied. Furthermore, the process of pore formation by chemical etching with hydrofluoric acid has been thoroughly investigated by assessing the effect of etchant concentration and etching time. The outcome of this investigation enables us to have precise control over the resulting geometry of nanopores arrays. As a result, guidelines for the creation of a-SiO 2 /Si templates with tunable parameters and general recommendations for their further application are presented.
Magnetic metal-oxide compounds with high values of magnetoresistance (MR) have attracted huge interest for spintronic applications, among which Sr2FeMoO6-δ (SFMO) has been relatively less known compared to the cobaltites and manganites, despite 100% electrons spin-polarization degree and a high Curie temperature. Here, stable fabrication and systematic analysis of nanocomposites based on SFMO with SrMoO4 dielectric sheaths are presented. SFMO-SrMoO4 nanocomposites were fabricated as follows: synthesis of the SFMO single-phase nanopowders by the modified citrate-gel technique; compaction under high pressure; thermal treatment for sheaths formation around grains. The nanocomposite is observed to exhibit a transitional behavior of conductivity from metallic, which is characteristic for the SFMO to semiconductor one in the temperature range 4 – 300K under magnetic fields up to 10T. A negative MR is observed due to the spin-polarized charge carriers tunneling through dielectric sheaths. MR value reaches 43% under 8T at 10κ. The dielectric sheaths thickness was determined to be about 10 nm by electric breakdown voltage value at current-voltage characteristics curves. The breakdown is found to be a reversible process determined by collisional ionization of dielectric atoms in strong electric field depending on knocked-out electrons from the SrMoO4. It was found that MR changes sign in electric breakdown region, revealing the giant magnetoresistive properties.
Nickel nanoparticles coated with few layers of carbon have been embedded into the polydimethylsiloxane (PDMS) matrix in concentrations up to 11 vol %. Dielectric and magnetic properties of composite materials have been studied in wide frequency (20 Hz–1 MHz) and temperature (130–430 K) ranges. It was demonstrated that the temperature behavior of dielectric properties is determined by glass transitions in the PDSM matrix below 200 K and the Maxwell–Wagner relaxation above room temperature. The possibility of using fabricated composites on the basis of the PDMS matrix for producing a wide range of passive electromagnetic components, such as frequency-selective filters, wide-band detectors/sensors of a bolometric type, and even electromagnetic “black holes” is also discussed.