In order to further theoretical and experimental research on adhesion recovery, an innovative new test-rig for wheel–rail contact experiments under large slip conditions was developed. The wheel-on-ring category of test-rig was determined to preserve surface conditions on rail. A scale factor of 1/4 and a circling diameter of 2 m were adopted considering the power limit in the laboratory and wheel–rail contact similarity. The test-rig consisting of wheel assemblies, ring track, gearbox, motors and sprinkler system was specially designed for motor decoupling and precise slip control. Then, the accuracy of slip under PID control was verified by simulation and experimental validation. Thereafter, experimental observations with different speeds, axle loads and surface contaminants showed the potential of the new test-rig for exploring adhesion recovery under various surface conditions.
The phenomenon of adhesion improvement during wheel-rail sliding has been experimentally verified under water conditions. However, the academic community is in agreement that, for oil that is also fluid, the adhesion characteristic curve under oil conditions exhibits a single peak, making adhesion improvement through wheel-rail sliding impossible. To investigate whether a similar adhesion improvement phenomenon exists under high-viscosity oil medium conditions as observed under water condition, this study conducted wheel-rail adhesion tests on oil-contaminated interfaces within a slip ratio up to 80%. The test results demonstrate that under higher wheel-rail slip, an adhesion improvement phenomenon also occurs on oil-contaminated rail surfaces, although it is more stringent compared to water conditions. The essence of this adhesion improvement is due to the lubrication failure of oil caused by temperature. Finally, this study analyzes the failure conditions of the oil-contaminated interface and its influencing factors, determining the thermal failure temperature range of the oil film.
Aiming at the problem of low control accuracy caused by nonlinear disturbances in the operation of the PLS-160 wheel–rail adhesion test rig, a linear active disturbance rejection controller (LADRC) suitable for the wheel–rail adhesion test rig was designed. The influence of nonlinear disturbances during the operation of the test rig on the control accuracy was analyzed based on SIMPACK. The SIMAT co-simulation platform was established to verify the control performance of the LADRC designed in this paper. The simulation results show that the speed and creepage errors of the test rig under the control of the LADRC met the adhesion test technical indicators under four different conditions. Compared with the traditional PID controller, the creepage overshoot and response time with the LADRC were reduced by 1.27% and 60%, respectively, under the constant creepage condition, and the stability recovery time was shorter under the condition of a sudden decrease in the adhesion coefficient. The LADRC designed in this paper shows better dynamic and anti-interference performance; therefore, it is more suitable for a follow-up study of the PLS-160 wheel–rail adhesion test rig.
Purpose: In response to the problem of insufficient traction/braking adhesion force caused by the existence of the third-body medium on the rail surface, this study aims to analyze the utilization of wheel-rail adhesion coefficient under different medium conditions and propose relevant measures for reasonable and optimized utilization of adhesion to ensure the traction/braking performance and operation safety of trains.Design/methodology/approach: Based on the PLS-160 wheel-rail adhesion simulation test rig, the study investigates the variation patterns of maximum utilized adhesion characteristics on the rail surface under different conditions of small creepage and large slip. Through statistical analysis of multiple sets of experimental data, the statistical distribution patterns of maximum utilized adhesion on the rail surface are obtained, and a method for analyzing wheel-rail adhesion redundancy based on normal distribution is proposed. The study analyzes the utilization of traction/braking adhesion, as well as adhesion redundancy, for different medium under small creepage and large slip conditions. Based on these findings, relevant measures for the reasonable and optimized utilization of adhesion are derived.Findings: When the third-body medium exists on the rail surface, the train should adopt the low-level service braking to avoid the braking skidding by extending the braking distance. Compared with the current adhesion control strategy of small creepage, adopting appropriate strategies to control the train’s adhesion coefficient near the second peak point of the adhesion coefficient-slip ratio curve in large slip can effectively improve the traction/braking adhesion redundancy and the upper limit of adhesion utilization, thereby ensuring the traction/braking performance and operation safety of the train.Originality/value: Most existing studies focus on the wheel-rail adhesion coefficient values and variation patterns under different medium conditions, without considering whether the rail surface with different medium can provide sufficient traction/braking utilized adhesion coefficient for the train. Therefore, there is a risk of traction overspeeding/braking skidding. This study analyzes whether the rail surface with different medium can provide sufficient traction/braking utilized adhesion coefficient for the train and whether there is redundancy. Based on these findings, relevant measures for the reasonable and optimized utilization of adhesion are derived to further ensure operation safety of the train.
To investigate the adhesion characteristics and sanding effect of rail vehicles on a contaminated rail surface, an innovative wheel/ring configuration test rig, named the PLS-Circulator, was employed. Based on the equivalence principle, the sanding condition relationship between the test rig and the field was first established. Then, extensive and quantitative experiments on the enhancement of rail vehicle adhesion in sanding conditions were conducted. The results show that the maximum adhesion coefficient of various media increases with an increase in the amount of sand, and the adhesion-enhancing effects gradually reach the threshold when the amount of sand is high. On the other hand, after a single application of sand, the increase in the adhesion coefficient gradually decreases over time, and the pattern of adhesion enhancement degradation varies in different media. It was found that oil is the most unfavorable condition, where the adhesion-enhancing effect deteriorates the fastest. The appropriate amount of sand on the PLS-Circulator is 0.3 g/m, corresponding to 4.8 g/m of sand in the field.
30 September 2025 in Advances in Mechanical Engineering
To address the low adhesion issue caused by contaminants such as water or oil entering the wheel-rail interface, high-speed rail vehicles utilize sanding devices to improve adhesion. This method effectively mitigates most low-adhesion conditions. However, subway vehicles currently lack sanding devices, leading to extended braking distances, wheel slip, and even collisions under low-adhesion conditions. This paper systematically investigates the wheel-rail adhesion change and the braking performance under the influence of sanding, aiming to explore the necessity of adding sanding devices to subway vehicles. Laboratory tests were conducted using a 1:4 circumferential test rig, which mimics the field lines, establishing an equivalence between the actual vehicle and laboratory conditions. The study also analyzed the deterioration of the sanding effect between Axles under three conditions: water, oil, and an oil/filings mixture. A subway braking/anti-slip simulation platform was developed, incorporating sanding deterioration, to evaluate the train braking performance under different sanding amount. Finally, the paper provides reasonable recommendations for the optimal installation positions of sand devices on subway vehicles.