Liquid metal embrittlement (LME) cracking is a phenomenon observed during resistance spot welding (RSW) of zinc−coated advanced high−strength steels (AHSS) in automotive manufacturing. In this study, severe cracks are observed at the edge of the sheet under reduced flange widths. These cracks, traversing the AHSS sheet, culminate at the edge with a width of approximately 1.2 mm. Through combined numerical and experimental investigations, and material testing, these cracks are identified and validated as a new type of LME crack. The mechanism behind this crack formation is attributed to unique geometric conditions that, when compared to center welding, amplify radial material flow by ninefold to 0.87 mm. The resultant tangential tensile stresses approximate 760 MPa, which exceed the yield strength of the examined advanced high−strength steel (AHSS) under heightened temperature conditions, and when combined with liquid zinc, promote the formation of this new type of LME crack.
The finite element analysis (FEA) simulation of directed energy deposition (DED) processes offers many potential cost savings during the build job optimization process, through, e.g., distortion predictions. However, the biggest challenge is the long calculation time, frequently exceeding the actual build time. One way of simplifying the simulation with the aim of reducing the calculation times is the inherent strain method. While this method is already used commercially in the simulation of powder bed-based processes and conventional welding technologies, its use in DED is still the subject of research. In this work, an inverse determination of an inherent strain is carried out on a 20-layer-high, single-track-wide wall, common theories are reviewed, and an approach based on thermal strain is introduced. As a result, the calculation time could be reduced by 83% and the accuracy remained at 92%.