In the automotive production line, a single pair of electrodes is employed to produce hundreds of consecutive welds before undergoing dressing or replacement. In consecutive resistance spot welding (RSW) involving Zn-coated steels, the electrodes undergo metallurgical degradation, characterized by Cu-Zn alloying, which impacts the susceptibility to liquid metal embrittlement (LME) cracking. In the present investigation, the possibility of LME crack formation in uncoated TRIP steel joints during consecutive RSW (involving 400 welds in galvannealed and uncoated TRIP steels) was investigated. The results have shown that different Cu-Zn phases were formed on the electrode surface because of its contamination with Zn from the galvannealed coating. Therefore, during the welding of the uncoated TRIP steel, the heat generated at the electrode/sheet interface would result in the melting of the Cu-Zn phases, thereby exposing the uncoated steel surface to molten Zn and Cu, leading to LME cracking. The cracks exhibited a maximum length of approximately 30 µm at Location A (weld center) and 50 µm at Location B (shoulder of the weld). The occurrence and characteristics of the cracks differed depending on the location as the number of welds increased due to the variation in Zn content. Type A cracks did not form when the number of welds was less than 280. Several cracks with a total length of approximately 30 μm were suddenly formed between 280 and 400 welds. On the other hand, type B cracks began to appear after 40 welds. However, the number and size of these exhibited inconsistency as the number of welds increased. Overall, the results have shown that small LME cracks can form even in uncoated steels during consecutive welding of Zn-coated and uncoated steel joints.
1 September 2025 in Journal of Materials Research and Technology
This study presents an inline quality inspection system for resistance spot welds that predicts nugget diameter and classifies surface defects using 3D scanning and machine learning. Indentation geometry data from a high-resolution 3D scanner are processed to extract 16 geometric features, analyzed by a hybrid model combining a convolutional neural network (CNN) and a rule-based algorithm. Surface defects are classified into six types: normal weld, edge weld, electrode tip degradation (ED), tilting, spatter, and pinhole, with ED divided into No ED, Low ED, and High ED based on its impact on weld quality. In inline operation, dual robots and a movable tracker cover the full body-in-white (BIW) within cycle time. The workflow integrates scanning, feature extraction, nugget prediction, and defect classification for immediate OK/NG decisions. A 3D visualization interface displays BIW components with color-coded weld status, process parameters, defect types, and ED levels, enabling rapid feedback. Validation with 62 specimens across various sheet combinations and field variables achieved high accuracy in both nugget prediction and defect classification, with an average inspection speed of 2.5 seconds per weld. This approach overcomes the limits of destructive and conventional non-destructive tests, offering a reliable inline solution for real-time feedback and smart factory implementation.