Cellulose hydrogels were prepared from commercial cellulose using NaOH/urea and LiCl/DMAc methods. For NaOH/urea method, alkali hydrates (OH-(H2O)x), urea hydrates (urea(H2O)y), and water were adsorbed into cellulose fiber to break hydrogen bonds between cellulose molecules yielding HG_Urea. For LiCl/DMAc method, the Lithium-DMAc complexes, [Li(DMAc)n]+Cl-, were seeped into cellulose fibers and the hydrogen bonds between the fibers were substituted by O-H…Cl-[Li(DMAc)n]+ bonds to produce transparent cellulose gel, HGL. Both freeze-dried hydrogels show the characteristics of cellulose vibrational modes and nano-sized fibrous SEM images. For water retention study, there was no significant difference when different amounts of HG_Urea were being used. Covering mung bean seeds directly helps improve the growth of roots, leaves and stems by 410, 28 and 27%, respectively. HGL and HGL in water were also tested on the germination of the mung bean seeds. As compared with HGL, the average lengths of roots, stems and leaves of mung bean on HGL-water were increased by 82, 32 and 14%, respectively
The Cordon of the Most Illustrious Order of Chulachomklao was one of the insignia that King Rama the fifth gave to the ladies of the court to present their goodness. One component of this object was made from silk and decorated by needled the silvered and golden thread as the laurel and the initial of King’s royal name. This ancient silk suffers from discoloration, low strength and severe deterioration. Amino acids in fibroin were photo-degraded under UV-irradiation and heat. Three silk samples, S-Raw, S-White and S-Ancient, were selected for ATR-FTIR and XRD analyses. FTIR spectroscopy can be used for the determination of the molecular structure of silk fibroin. The characteristic bands of silk fibroin corresponding to amide I, II, and III were found in all silk samples. The skeletal vibrations were also observed. Two degradation estimators, EAmideI/II and EcC=O2 were calculated and used to qualitatively estimate the degree of degradation due to oxidation and crystallinity of silk fibroin respectively. The results showed the higher degree of degradation and lower crystallinity of A-Ancient. The X-ray diffraction of S-Ancient showed the broader and weaker characteristic peaks at 2 theta of ∼ 20o indicating the lower crystallinity.