Aluminum alloy processing via additive manufacturing (AM) technologies has increased in usage during the last decade. AM now enables manufacturing complex geometries not previously achieved through traditional manufacturing. Aluminum is usually processed using laser powder bed fusion (LPBF) technologies, which are used to manufacture metallic components of high geometrical complexity and dimensional accuracy and good mechanical, electrical, and chemical properties, which is why this technology is quite popular at industrial levels. To further develop quality control systems and new aluminum alloys using LPBF, there is a need to establish a predictive relationship between the parameters of the material. A study was carried out to investigate the relationship between energy density and process parameters such as laser power, scan speed, hatch spacing, scan pattern, and laser focus and its influence on the densification mechanism in additively manufactured components with aluminum alloys. AA6061 was selected due to its wide usage in different industries, given its low density and high mechanical performance. Relative density was analyzed using the Archimedes principle, and the quality and morphology of the AA6061 powder were analyzed through metallographic analysis. The process parameter selection was performed according to the best results obtained according to the laser power and energy density factors. The best manufactured samples had an energy density between 30 and 40 J/mm3, with relative densities above 99%.
En esta investigación se llevó a cabo una caracterización mecánica de dos tipos de materiales compuestos: resina poliéster reforzada con fibra de vidrio y resina poliéster reforzada con fibra de bambú. Se realizaron ensayos de tracción, flexión e impacto siguiendo las normas internacionales ASTM. Las fibras de bambú fueron obtenidas de forma manual y para mejorar la compatibilidad matriz de poliéster/ fibra, fueron sometidas a un tratamiento químico con hidróxido de sodio al 5 % en masa. Las muestras fueron elaboradas con concentraciones en masa de fibras de bambú de 11.07, 13.53 y 16.23 % y para poliéster reforzado con fibras de vidrio de 10.11, 14.77 y 19.19 %. Las propiedades mecánicas de estos materiales compuestos fueron comparadas con la matriz de poliéster sin refuerzo con el fin de conocer el aporte mecánico que le hacen las fibras a la matriz.