Yan Ma

Dr. Yan Ma

orcid

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
19 July 2017 in Scientific Reports
Verified
Journal Article
Open access
PDF file
QGQiuzhi Gao
Qiuzhi Gao
YZYanan Zhang
Yanan Zhang
HZHailian Zhang
Hailian Zhang
Huijun LiHuijun Li
Huijun Li
FQFu Qu
Fu Qu
YMYan Ma
Yan Ma
The precipitates obtained by EPE technology from the 9Cr-1.7W-0.4Mo-Co ferritic heat-resistant steel subject to isothermal aging were investigated using SEM, TEM and XRD. The particle size distribution and the coarsening kinetics of M23C6 with duration of isothermal aging were also analyzed with or without consideration of Laves phase. The results show that the isolated dislocations were detected in delta ferrite interior, and the precipitates on delta ferrite and martensite boundaries are obviously larger than other locations. Fe2W-Laves phase can only be found as duration of aging time to 2000 h, and is preferential to form adjacent to M23C6 particles. The small M23C6 particles firstly coarsen, but the large M23C6 are relatively stable during short aging. The total coarsening rate of M23C6 precipitates is 9.75 × 10−28m3s−1, and the coarsening of M23C6 depends on the formation of Laves phase.

16 December 2023 in Metals
Verified
Journal Article
Open access
PDF file
YMYan Ma
Yan Ma
Lihong SuLihong Su
Lihong Su
CSChen Shen
Chen Shen
LFLeigh Fletcher
Leigh Fletcher
Huijun LiHuijun Li
Huijun Li
CZChuanguo Zhang
Chuanguo Zhang
The low-temperature fracture toughness of double-V weld seams is a well-known challenge due to the essential increased heat input for heavy-wall pipelines. A thorough investigation was conducted to explore the impact of the heat input on the grain size and precipitate coarsening, correlating the microstructure with the heat-affected-zone (HAZ) toughness. The results indicated that the actual weldments showed a toughness transition zone at −20 °C, with considerable scattering in Charpy V-notch (CVN) tests. Gleeble thermal simulations confirmed the decreased toughness of the coarse-grained HAZ (CGHAZ) with increasing heat input and prior austenite grain size (PAGS). A specially designed thermal treatment demonstrated its potential for enhancing the toughness of the CGHAZ, with the recommended thermal cycle involving peak temperatures of 700 and 800 °C, holding for 1 s, and rapid cooling. The toughness of the intercritically reheated CGHAZ (ICCGHAZ) improved with higher intercritical reheating temperatures and the removal of necklace-type M–A constituents along the PAG. Despite various thermal treatments, no significant improvements were observed in the toughness of the ICCGHAZ. Future work was suggested for optimising the use of tack welds to reduce the effective heat input (HI) associated with double-sided submerged arc welding (SAW).

27 September 2023 in Science China Materials
Verified
Journal Article
Open access
PDF file
ZWZhanxin Wang
Zhanxin Wang
YGYizhong Guo
Yizhong Guo
YMYan Ma
Yan Ma
CYChengpeng Yang
Chengpeng Yang
YZYadi Zhai
Yadi Zhai
XHXiaodong Han
Xiaodong Han

摘要

非共格孪晶界(ITB)能显著影响金属力学性能, 受到了研究者极 大关注. 理论模型预测ITB是由系列偏位错组成, ITB两侧的晶面没有 沿[111]方向的相对位移. 本文利用分子静力学模拟研究了Ag, Cu, Ni 和Al中ITB的结构, 发现ITB的结构具有显著的尺寸效应. 对于较薄的 ITB, 界面两侧的晶面处于同一水平面, 没有沿[111]方向的相对位移, 与理论模型结果一致. 而对于较厚的ITB, 界面两侧的晶面有明显的 [111]方向的相对位移, 且相对位移随着ITB厚度的增加而增加. 此外, 研究揭示出ITB两侧晶面沿[111]方向的位移与金属的层错能直接相关. 该研究表明ITB的结构并不唯一, 不同的厚度、层错能对应不同的ITB 结构. 本研究为理解孪晶厚度和层错能对金属力学性能的影响提供了 新见解.


11 June 2024 in Materials
Verified
Journal Article
Open access
PDF file
ZZzhihao zhang
zhihao zhang
YMYan Ma
Yan Ma
SLShuo Liu
Shuo Liu
Lihong SuLihong Su
Lihong Su
LFLeigh Fletcher
Leigh Fletcher
Hongtao ZhuHongtao Zhu
Hongtao Zhu
Unforeseen failures in girth welds present a significant challenge for the pipeline industry. This study utilizes 3D Digital Image Correlation (DIC) assisted cross-weld tensile testing to analyze the strain response of high-strength thick-walled pipelines, providing essential insights into the strain migration and fracture mechanisms specific to girth welds. The results reveal that the welding process significantly affects the mechanical distribution within the girth weld. The tested Shielded Metal Arc Welded (SMAW-ed) pipe exhibited undermatched girth welds due to high heat input, while Gas Metal Arc Welding (GMAW) introduced a narrower weld and Heat-Affected Zone (HAZ) with higher hardness than the base metal, indicative of overmatched girth welds. Strain migration, resulting from a combination of metallurgical heterogeneous materials and geometrical reinforcement strengthening, progressed from the softer HAZ to the base metal in the SMAW-ed sample with reinforcement, ultimately leading to fracture in the base metal. In contrast, the GMAW-ed sample shows no strain migration. Reinforcement significantly improves the tensile strength of girth welds and effectively prevents failure in the weld region. Sufficient reinforcement is crucial for minimizing the risk of failure in critical areas such as the weld metal and HAZ, particularly in SMAW-ed pipes.

18 August 2023 in Wear
Verified
Journal Article
Closed access
BNBa Hieu Nguyen
Ba Hieu Nguyen
ECEduardo Tovar Camacho
Eduardo Tovar Camacho
AAAli Al-Juboori
Ali Al-Juboori
YMYan Ma
Yan Ma
Huijun LiHuijun Li
Huijun Li
Hongtao ZhuHongtao Zhu
Hongtao Zhu

20 November 2024
Verified
Book Chapter
Closed access
PDF file
TZTianhao Zhou
Tianhao Zhou
ZQZhijun Qiu
Zhijun Qiu
YLYuxing Li
Yuxing Li
YMYan Ma
Yan Ma
WTWei Tao
Wei Tao
Huijun LiHuijun Li
Huijun Li
In this study, wire arc additive manufacturing (WAAM) process is used to build the nickel-based Inconel 718 superalloy (IN718) and stainless-steel 316L (SS316L) bimetallic components with an interweaving building strategy in a cost-effective manner. The bimetallic wall structures are built with different welding parameters, aiming to investigate the feasibility of fabricating a bimetallic component using these two alloys. The results show that typical columnar grains with elongated dendrites characterised the matrix of the manufactured components. A number of cracks are found in the interface between the two materials and mostly in the SS316 site of those samples; nevertheless, the enhanced cooling rate appeared to decrease cracks. In addition, the as-fabricated samples have a similar hardness value to the WAAM process fabricated IN718 and SS316, respectively. Based on the small punch test (SPT), the tensile properties of the samples are comparable to that of commercial stainless steel, and the fracture area of SPT is generally on the steel side. This research provides valuable knowledge in process parameters to produce high-quality IN718-SS316L bimetallic complex geometric components via WAAM to meet the demand for joining highly alloyed materials for specific structural applications. <!----> <!----> <!----> <!---->