Purpose. One of the most common problems in mechanized excavation is the cutting tool wear, which has a great impact on the final cost of the project and its duration. Also, one of the most important factors affecting the wear of cutting tools is the operating parameters of the tunnel boring machine (TBM). Within the framework of this research, a tunnel boring machine laboratory simulator was designed and constructed to investigate the tunnel excavation process in the laboratory. Methods. A few of the features of this device are that it operates horizontally, has a low rotation speed, keeps the pins in contact with fresh soil throughout the test, and has the possibility of measuring the torque of the device during the test. A study of the cutting tool wear was conducted using granulation prepared from Tabriz metro line 2, as well as using operating parameters of mechanized excavation machines, such as penetration rate and cutter head rotation speed. Findings. The research results showed that by reducing the rotation speed of the cutter head from 35 to 10 rpm, the average wear of cutting tools is reduced by 63%. Also, by reducing the excavation time from 80 to 10 minutes, the cutting tool wear is reduced by 58%. The wear of cutting tool increases with increasing moisture content from 0 to 10%, and then decreases with increasing moisture content from 10 to 25%. Originality. During this research, a new device was designed and built to simulate tunnel excavation mechanisms. This laboratory simulator measures wear percentage, penetration rate and torque. Practical implications. There has been significant progress in predicting soil abrasion rates, but there are few accepted models for predicting cutting tool wear and soil abrasion rates. During the design and construction of the tunnel boring machine laboratory simulator, the effect of operating parameters on wear of cutting tool was examined.
Evaluation of the cutting and wear performance of cutting tools in full-face tunnel boring machines (TBMs) for soil and rock formations is critical for accurate project scheduling and cost estimation. The significant investment costs associated with mechanized tunneling necessitate comprehensive laboratory and numerical tests, such as linear cutting tests, to guide machine selection and cutterhead configuration. This study investigates the performance of cutting tools using a novel small-scale Linear Cutting Machine (LCM). To achieve this, a small-scale LCM was developed, and linear cutting tests were performed on nine rock specimens of varying geological origins. Each rock specimen measured 200 mm × 150 mm × 80 mm. The shear disk studied in this research is located 3.5 m from the center of the cutterhead. This shear disk travels a distance of 22 m with each rotation of the TBM cutterhead, considering the circumference of the circle. Based on the 1:10 scale conversion applied in this study, the constructed shear disk should also travel 2.2 m across the rock. Several cutting components are analyzed in linear cutting tests, including specific energy (SE), cutting coefficient (CC), and disk wear. Additionally, all laboratory tests were numerically modeled using the finite element method under identical boundary conditions. Results indicated that Basalt-1, due to its high porosity, required the highest specific energy, while softer rocks like travertine-1 exhibited the lowest. Also, the cutting coefficient increased with penetration depth, emphasizing its role in controlling friction and optimizing disc bearing performance. Fossiliferous limestone demonstrated the highest cutting coefficient due to its fine-grained structure and high friction. Identifying penetration depths that maximize excavation rates while minimizing forces, this study enhanced excavation efficiency and tool longevity.
Cutting tool resistance to abrasion are among the most important factors in the efficiency of earth pressure balance (EPB)–tunnel boring machines (TBMs). Excessive wear negatively affects the operating parameters of the tunneling machine and reduces its efficiency. Considering the lack of a comprehensive and accepted method for the study of wear in soft grounds, this study sought to design and manufacture a TBM tunneling simulator to better understand the interaction between soil and cutting tools. For this purpose, after introducing a new machine manufactured in Sahand University of Technology (Tabriz, Iran), the effect of the density of two types of soil with different granulation and moisture on the wear of cutting tools under different conditions was investigated to simulate the TBM tunneling mechanism. The low rotational speed of the cutterhead (similar to EPB machines), continuous contact of the cutting tool with the intact soil, continuous injection of conditioning additives with specified injection pressure during the test, and horizontal operation similar to TBM are the most important features of this machine. The results indicated that an increase in the soil density from 1.5 to 2.0 g/cm3 at a moisture content of 7 % increased the maximum wear of cutting tools from 4.1 to 11.6 %. Accordingly, a similar trend was observed for moisture of 13 %. By studying wear at different densities and percentages of moisture, a decreasing trend of wear was observed under the same conditions at a higher moisture percentage. Furthermore, increasing the soil density initially increases the wear of cutting tools, although a further increase in the density causes clogging in the cutterhead, and no significant changes were observed in the amount of wear in this area. Finally, the results of some operational tests show that increasing the penetration rate and rotational speed of the cutterhead can decrease and increase tool wear under different conditions, respectively.
In a natural condition, temperature variations and phase transition of pore water are the two most effective factors on the mechanical properties of rocks. Instabilities occurred as a result of climate changes, highlight the importance of rock characteristics. This paper conducted a laboratory investigation to study the temperature-dependent mechanical behavior of rocks and to examine the quantity and quality of this relationship. In order to perform laboratory tests, a temperature-controlling apparatus was developed. Studies were conducted on 152 specimens of concrete and three types of rocks, including granite, red travertine, and walnut travertine. Then, the effect of temperature variations, from -30 to +30ºC with 10ºC intervals on the mechanical properties of the rocks, was studied. The results showed that temperature reduction, caused by pore water phase transition, improved the mechanical properties of the rocks. The maximum variation of the mean uniaxial compressive strength from +30ºC to -30ºC belonged to granite (40.1%), while the concrete specimen showed the minimum variation on the test results (33.7%). Red travertine (38.7%) and walnut travertine (34.2%) exhibited lower variations compared to granite. Also, the maximum variation in the mechanical behavior of rocks occurred between -10 and 0 °C. Additionally, variations in the mechanical properties of cracked rock samples were more than the rocks with spherical pore and the same porosity percent.
1 January 2023 in Rudarsko-geološko-naftni zbornik
The lining system, used in tunnel boring machines, is made of precast concrete segments. The use of steel fibers in this kind of support system can not only decrease production time and costs but also can improve compressive, tensile as well as flexural behaviors. A study has been carried out to examine the mechanical properties of segments in the Tabriz metro line-2 project using three types of steel fibers: 3D, 4D, and 5D. Various experiments were investigated to monitor the workability of Steel Fiber Reinforced Concrete (SFRC) under various loads. The results confirmed an improvement in the specimens’ mechanical properties because of these types of steel fibers. 5D, 4D, and 3D fibers provided the greatest effect on the tensile and flexural strength of steel fiber-reinforced concrete, respectively. The 28-day compressive, tensile, and flexural strengths of the specimens are incremented by 13%, 68%, and 154%, respectively. In addition, by conducting tests on the orientation of steel fibers, placing the fibers perpendicular to the load can improve the compressive strength of concrete by almost 18%.